1.
Odovtos (En línea) ; 25(3): 55-66, Sep.-Dec. 2023. tab, graf
Artigo em Inglês | LILACS, SaludCR | ID: biblio-1529069

RESUMO

Abstract To evaluate the accuracy of complete arch scanning with multiple implant titanium scan bodies using laboratory scanners. A master model of an edentulous maxillary arch with 6 implants was fabricated. Titanium scan bodies were inserted into the model. Three laboratory scanners were used: D2000 (3Shape), Vinyl High Resolution (Smart Optics), and inEos X5 (Dentsply Sirona). The master model was consecutively scanned ten times using dental laboratory scanners (LS) without detaching and repositioning the scan bodies. Linear and angular accuracy between adjacent implants was measured using inspection software (Control X, Geomagic). The accuracy of the complete arch scans was calculated. Implant regions were defined as; parallel (R1: #24-26 and #16-14), angled (R2: #22-24 and #14-12), angled to occlusal plane (R3: #12-22), and cross-arch (R4: #16-26). The effect of LS and implant region on accuracy was compared using two-Way ANOVA (α=0.05). Significant greater linear distortion was noted in R4 (61.2±17.9µm) compared to R1 (23.4±15.5µm) and R2 (26±17.7µm) (p<0.01). Greater linear distortions were noted in R4 with D2000 (0.07±0.016 degrees) and Vinyl High Resolution (0.067±0.02 degrees) than inEos X5 (0.032±0.021 degrees) (p>0.05). Greater mean linear precisions were noted in R1 (9±8µm) and R3 (9.3±8.3µm) than R4 (12.6±10.3µm) (p<0.05). The highest linear precision was noted in D2000 (7.2±7.6µm) (p<0.05). The angular precision of D2000 (0.02±0.015 degrees) was the highest (p<0.01). The angular precisión of R4 (0.036±0.018 degrees) was the lowest (p<0.01). This study revealed that the trueness was affected by the implant region and the precision was affected by both LS and implant region.


Resumen Evaluar la precisión del escaneado de la arcada completa con cuerpos de escaneado de titanio de múltiples implantes utilizando escáneres de laboratorio. Se fabricó un modelo maestro de una arcada maxilar edéntula con 6 implantes. Se insertaron cuerpos de escaneo de titanio en el modelo. Se utilizaron tres escáneres de laboratorio: D2000 (3Shape), Vinyl High Resolution (Smart Optics) e inEos X5 (Dentsply Sirona). El modelo maestro se escaneó consecutivamente diez veces usando escáneres de laboratorio dental (LS) sin separar y reposicionar los cuerpos de escaneo. La precisión lineal y angular entre implantes adyacentes se midió utilizando un software de inspección (Control X, Geomagic). Se calculó la precisión de los escaneos completos del arco. Las regiones del implante se definieron como; paralelo (R1: #24-26 y #16-14), angulado (R2: #22-24 y #14-12), angulado al plano oclusal (R3: #12-22) y cruzado (R4: #16-26). El efecto de LS y la región del implante en la precisión se comparó mediante ANOVA de dos vías (α=0,05). Se observó una distorsión lineal significativamente mayor en R4 (61,2±17,9µm) en comparación con R1 (23,4±15,5µm) y R2 (26 ±17,7µm) (p<0,01). Se observaron mayores distorsiones lineales en R4 con D2000 (0,07±0,016 grados) y vinilo de alta resolución (0,067±0,02 grados) que en inEos X5 (0,032±0,021 grados) (p>0,05). Se observaron precisiones lineales medias mayores en R1 (9±8µm) y R3 (9,3±8,3µm) que en R4 (12,6±10,3µm) (p<0,05). La mayor precisión lineal se observó en D2000 (7,2±7,6 µm) (p<0,05). La precisión angular de D2000 (0,02±0,015 grados) fue la más alta (p<0,01). La precisión angular de R4 (0,036±0,018 grados) fue la más baja (p<0,01). Este estudio reveló que la veracidad se vio afectada por la región del implante y la precisión se vio afectada tanto por LS como por la región del implante.


Assuntos
Titânio , Implantes Dentários , Tomógrafos Computadorizados , Arco Dental/diagnóstico por imagem
2.
Odontol. vital ; (39): 27-39, jul.-dic. 2023. tab, graf
Artigo em Espanhol | LILACS, SaludCR | ID: biblio-1550585

RESUMO

RESUMEN Introducción: Los tratamientos para fracturas de órbita se basan en la corrección del defecto de las lesiones orbitarias de tipo blow in y blow out (o de estallido), mediante diversas placas y mallas biocompatibles con el organismo, dándose una cicatrización de primera generación evitando un callo óseo y una fijación más rígida. Para el diagnóstico de este tipo de lesiones tenemos inflamación periorbitaria, enoftalmos, diplopía, equimosis, hemorragia subconjuntival. Existen diversos materiales reconstructivos siendo estos compuestos por distintas materias primas, como son los aloplásticos y autógenos; donde encontramos varios tipos como placas de titanio y las placas reabsorbibles siendo estas las más comunes y usadas actualmente, por su bajo estímulo a reabsorciones óseas y evitando efectos secundarios a largo plazo. Estas placas presentan diversos grados de ductilidad y resistencia. Se informó sobre varias complicaciones según el tipo de placas como es la cicatrización, las cirugías postquirúrgicas en caso de placas de titanio, etc. El objetivo de esta revisión es la evaluación de la eficacia las placas reabsorbibles versus placas de titanio en fracturas de órbita. Materiales y métodos: La investigación es de carácter documental, descriptivo y no experimental. En el cual se emplea una metodología de identificación e inclusión de artículos científicos tipo prisma. Resultados y conclusiones: Se verificaron las ventajas y desventajas tanto de las placas reabsorbibles como las de titanio siendo estas similares en la biocompatibilidad con el organismo humano, así como también varias diferencias como el soporte, fuerzas, resistencia de estas, concluyendo que es debatible el material ideal para tratar fracturas de órbita. Se seleccionaron artículos tomando en cuenta el título y objetivos; considerando estudios comparativos, revisiones sistemáticas, revisiones de literatura, los cuales comprendían criterios con respecto a fracturas de órbita y tratamientos quirúrgicos. La búsqueda arrojó 55 artículos en PubMed, 65 en Google, 4 en Scielo y 29 en Science direct, de los cuales se excluyeron libros, monografías, estudios experimentales, dando como resultado 21 artículos para el desarrollo de esta revisión bibliográfica. Y que fueron leídos y analizados en su totalidad, estudiando los objetivos, metodología y conclusión de cada uno de ellos para la posterior comparación.


ABSTRACT Introduction: Treatments for orbit fractures are based on the correction of the defect of blow in and blow out orbital injuries, by means of various plates and meshes biocompatible with the organism, giving a first-generation healing avoiding a bony callus and a more rigid fixation. For the diagnosis of this type of lesions we have periorbital inflammation, enophthalmos, diplopia, ecchymosis, subconjunctival hemorrhage. There are several reconstructive materials being these composed of different raw materials, such as alloplastic and autogenous, where we find several types such as titanium plates and resorbable plates being these the most common and currently used, for its low stimulus to bone resorption and avoiding long-term side effects. These plates have different degrees of ductility and resistance. Several complications have been reported depending on the type of plates, such as scarring, post-surgical surgeries in the case of titanium plates, etc. The objective of this review is to evaluate the efficacy of resorbable versus titanium plates in orbital fractures. Materials and methods: This research are a documentary, descriptive and non-experimental nature. A prism-type methodology of identification and inclusion of scientific articles was used. Results and conclusions: The advantages and disadvantages of both resorbable and titanium plates were verified, being these similar in biocompatibility with the human organism, as well as several differences such as support, forces, resistance of the same, concluding that it is debatable. The ideal material to treat orbital fractures. Articles were selected considering the title and objectives; considering comparative studies, systematic reviews, literature reviews, which included criteria regarding orbital fractures and surgical treatments. The search yielded 55 articles in PubMed, 65 in Google, 4 in Scielo and 29 in Science direct, from which books, monographs, experimental studies were excluded, resulting in 21 articles for the development of this bibliographic review. The 21 articles were read and analyzed in their entirety, studying the objectives, methodology and conclusion of each one of them for subsequent comparison.


Assuntos
Humanos , Órbita/lesões , Placas Ósseas , Titânio , Materiais Biocompatíveis/uso terapêutico , Fraturas Ósseas/cirurgia
3.
Int. j. morphol ; 41(5): 1317-1322, oct. 2023. ilus, tab
Artigo em Inglês | LILACS | ID: biblio-1521018

RESUMO

SUMMARY: Traumatized bone tissue has the capacity to repair itself so that it eventually regains its almost original form, even in the case of artificially inserted implants. The process that stays at the base of the regeneration is represented by osteogenesis or remote osteogenesis. The major difference between the two types of bone formation is the location of the cement line, which is located on the surface of the implant for contact osteogenesis and on the surface of the bone defect for remote osteogenesis. The aim of the present study was to assess the contact osteogenesis in the case of inserted titanium screws in holes with diameters of 1.8 mm and 1 mm respectively. The obtained results show, in the case of the groove with 1.8 mm that the newly proliferated bone represents 73.85 % of the total area, while in the case of the groove with 1 mm in diameter the value of the newly proliferated bone is 26.15 %. In conclusion, the insertion of titanium screws by self-tapping into the hole smaller than the core of the screw is accompanied by bone proliferation by contact osteogenesis much more modest than in the case of insertion into the hole larger than the core of the screw.


El tejido óseo traumatizado tiene la capacidad de reparar en forma espontánea, de modo que eventualmente recupera su forma casi original, incluso en el caso de implantes insertados artificialmente. El proceso que queda en la base de la regeneración está representado por la osteogénesis u osteogénesis a distancia. La principal diferencia entre los dos tipos de formación ósea es la ubicación de la línea de cemento, que se encuentra en la superficie del implante para la osteogénesis de contacto y en la superficie del defecto óseo para la osteogénesis remota. El objetivo del presente estudio fue evaluar la osteogénesis de contacto en el caso de tornillos de titanio insertados en forámenes con diámetros de 1,8 mm y 1 mm respectivamente. Los resultados obtenidos muestran, en el caso del surco de 1,8 mm que el hueso neoproliferado representa el 73,85 % del área total, mientras que en el caso del surco de 1 mm de diámetro el valor del hueso neoproliferado es del 26,15 %. En conclusión, la inserción de tornillos de titanio por autorroscantes en el foramen menor que el núcleo del tornillo se acompaña de una proliferación ósea por osteogénesis de contacto mucho más modesta que en el caso de la inserción en el foramen mayor que el núcleo del tornillo.


Assuntos
Animais , Masculino , Coelhos , Osteogênese , Próteses e Implantes , Titânio/química , Parafusos Ósseos , Osseointegração
4.
RFO UPF ; 28(1)20230808. ilus
Artigo em Português | LILACS, BBO - Odontologia | ID: biblio-1511056

RESUMO

Introdução: Mesmo com toda evolução tecnológica desses instrumentos, com o desenvolvimento das limas de liga de níquel-titanio (NiTi) e sistemas mecanizados, as fraturas podem ocorrer durante o preparo químico/mecânico. Existem três abordagens mais regulamente aplicadas para solucionar essa intercorrencia: tentativa de remoção do instrumento com ultrassom, tentativa de ultrapassálo (bypass) ou a obturação do segmento. Objetivo: Relatar um caso da técnica de bypass em instrumento fraturado no canal radicular. Descrição do caso: Paciente, sexo feminino, 47 anos, brasileira, sem condições sistêmicas associadas, foi encaminhada à clínica do Curso de Odontologia da UNIFENAS, Divinópolis, Minas Gerais, Brasil, para resolução de fratura de instrumento no canal mésio- vestibular do primeiro molar superior direito (16). Optou-se pelo tratamento pela técnica de bypass, que envolveu as seguintes etapas: anestesia, abertura, utilização de lima C-Pilot #08 para ultrapassar o instrumento fraturado, odontometria, escalonamento regressivo a partir da lima k#20, desinfecção com hipoclorito de sódio 5%, medicação com hidróxido de cálcio por 21 dias, agitação da substância irrigadora e obturação dos canais radiculares. Conclusão: O bypass ao instrumento é uma técnica conservadora, eficaz e uma solução adequada em casos de fratura de limas endodônticas dentro dos canais radiculares. Essa técnica visa preservar o máximo possível da estrutura dental original, evitando procedimentos mais invasivos.(AU)


Introduction: Even with all technological evolution of these instruments, with the development of nickel-titanium alloy (NiTi) files and mechanized systems, fractures can occur during chemical/mechanical preparation. There are three most commonly applie to resolve this complication: attempting to remove the instrument with ultrasound, attempting to bypass it, or obturating the segment. Objective: To report a case of bypass technique in fractured instrument in the root canal. Case description: A 47-year-old female patient from Brazil, with no associated systemic conditions, was referred to the clinic of the Dentistry Course at UNIFENAS, Divinópolis, Minas Gerais, Brazil, for resolution of an instrument fracture in the mesio-vestibular canal of the right upper first molar (16). Treatment was performed using the bypass technique, which involved the following steps: anesthesia, opening, use of a C-Pilot #08 file to bypass the fractured instrument, odontometry, regressive scaling from the k#20 file, disinfection with 5% sodium hypochlorite, medication with calcium hydroxide for 21 days, agitation of the irrigating substance and root canal filling. Conclusion: Instrument bypass is a conservative, effective technique and an adequate solution in cases of endodontic file fracture within root canals. This technique aims to preserve as much of the original tooth structure as possible, avoiding more invasive procedures.(AU)


Assuntos
Humanos , Feminino , Pessoa de Meia-Idade , Tratamento do Canal Radicular/instrumentação , Instrumentos Odontológicos , Cavidade Pulpar/diagnóstico por imagem , Falha de Equipamento , Titânio , Radiografia Dentária , Resultado do Tratamento , Níquel
5.
Braz. dent. sci ; 26(4): 1-9, 2023. ilus, tab
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-1523759

RESUMO

Introduction: The development of new biomaterials with improved properties is a trend in regenerative medicine. The successful healing of implants is related to their osseointegration and the topographic geometry of their surface. Treatment with argon plasma acts on the surface of the implants, bringing several benefits to their osseointegration in the body. Material and Methods: Previously the in vivo study, the topography implants were observed by scanning electron microscopy (SEM). Following the implants were inserted in 14 male rats, and one perforation was made in the right and left tibias for implant placement without the surface treatment (control group), and with the argon plasma surface treatment (experimental group), respectively. The rats were euthanized at 4 weeks, a time in which tibia fragments were submitted for histological and histomorphometric examination, and torque removal test for comparison and analysis of osseointegration. Results: The SEM images showed the argon plasma surface treatment altered the topography. At the end of the study, both greater bone formation and better osseointegration were verified in the experimental group, and a statistically significant difference between the groups was observed. Conclusion: It was concluded that implants with this surface treatment can bring more practicality in the rehabilitation treatment, and more comfort in the patients' postoperative time (AU)


Introdução: O desenvolvimento de novos biomateriais com propriedades aprimoradas é uma tendência na medicina regenerativa. A cicatrização bem-sucedida dos implantes está relacionada à sua osseointegração e à geometria topográfica de sua superfície. O tratamento com plasma de argônio atua na superfície dos implantes, trazendo diversos benefícios para sua osseointegração no corpo. Materiais e Métodos: Antes do estudo in vivo, a topografia dos implantes foi observada por microscopia eletrônica de varredura (MEV). Em seguida, os implantes foram inseridos em 14 ratos machos, e uma perfuração foi feita nas tíbias direita e esquerda para a colocação do implante sem o tratamento de superfície (grupo controle) e com o tratamento de superfície de plasma de argônio (grupo experimental), respectivamente. Os ratos foram sacrificados após 4 semanas, momento em que fragmentos das tíbias foram submetidos a exame histológico e histomorfométrico, além do teste de remoção de torque para comparação e análise da osseointegração. Resultados: As imagens de MEV mostraram que o tratamento de superfície com plasma de argônio alterou a topografia. Ao final do estudo, foi verificada maior formação óssea e melhor osseointegração no grupo experimental, e foi observada diferença estatisticamente significativa entre os grupos. Conclusão: Concluiu-se que os implantes com esse tratamento de superfície podem trazer mais praticidade no tratamento de reabilitação e maior conforto no pós-operatório dos pacientes (AU)


Assuntos
Animais , Ratos , Titânio , Implantes Dentários , Osseointegração , Torque
6.
Braz. dent. sci ; 26(4): 1-10, 2023. ilus, tab
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-1523860

RESUMO

Objective: The aim of this in vitro study w as t o analyze the influence of the titanium dioxide nanotubes i n a self-cure mode polymerization of a dual resin luting agent through push out bond strength and radiopacity tests. Material and Methods: After mixed with a commercial du al self-adhesive resin cement, three concentrations o f tit anium dioxide nanotubes (0.3, 0.6, and 0.9% by weight) we re analyzed in self-curing mode. T he bond strength to bovine root dentin and fi berglass posts was assessed with the push out bond str ength t est and was evaluated in three thirds (cervical, middle and apical) (n=10), followed by failure mode analysis (SEM), and the ISO standard 9917-2 was followed for radiopacity test (n=10). Data were statistically analyzed by one-way ANOVA test, followed by Tukey's test (α=0.05). Results: Reinforced self-adhesive resin cement with 0.6% titanium dioxide nanotubes showed significant difference compared to the control gr oup for push out test (p=0.00158). The modified groups did not s how significant difference among thirds (p=0.782). Radiopacity sh owed higher value for group w ith 0.9% titanium dioxide nanotubes in comparison w ith control group (p<0.001). Conclusion: The addition of titanium dioxide nanotubes to a self-adhesive resin cement increased the bond strength to dentin and radiopacity values in the self-cure polymerization mode (AU)


Objetivo: O objetivo deste estudo in vitro foi analisar a influência de nanotubos de dióxido de titânio na polimerização química de um agente cimentante resinoso dual através de testes de resistência à união e radiopacidade. Material e Métodos: Após misturado com um cimento resinoso auto-adesivo comercial, três concentrações de nanotubos de dióxido de titânio (0,3, 0,6 e 0,9% em peso) foram analisadas. A resistência da união para a dentina da raiz bovina e os pinos de fibra de vidro foi avaliada pelo teste de push-out e avaliada em três terços (cervical, médio e apical) (n = 10), seguido pelo análise de modo de falha (MEV) e a norma ISO 9917-2 foi seguido para teste de radiopacidade (n = 10). Os dados foram analisados estatisticamente pelo teste ANOVA um fator seguido do teste de Tukey (α = 0,05). Resultados: O cimento resinoso auto-adesivo reforçado com nanotubos de dióxido de titânio a 0,6% mostrou diferença significativa em comparação com o grupo controle para teste de push-out (p=0,00158). Os grupos modificados não mostraram diferença significativa entre os terços (p=0,782). A radiopacidade mostrou maior valor para o grupo com nanotubos de dióxido de titânio 0,9% em comparação com o grupo controle (p<0,001). Conclusão: A adição de nanotubos de dióxido de titânio a um cimento resinoso auto-adesivo aumentou a os valores de resistência de união à dentina e radiopacidade no modo de polimerização química do agente cimentante (AU)


Assuntos
Titânio , Cimentos Dentários , Pinos Dentários , Nanotubos
7.
Rev. odontol. UNESP (Online) ; 52: e20230021, 2023. ilus
Artigo em Português | LILACS, BBO - Odontologia | ID: biblio-1530303

RESUMO

Introdução: A importância da rugosidade para a osseointegração se dá pela correlação das interações das proteínas com a superfície do implante, a adsorção. Diferentes métodos são utilizados nos tratamentos de superfície, em que ocorre a remoção de partes da camada superficial, como o ataque ácido. Objetivo: Analisar as alterações de rugosidade na superfície dos implantes osseointegrados tratadas por duplo ataque ácido com uso único e até quatro reutilizações dos ácidos. Material e método As amostras de implantes dentários de liga de titânio (SINGULAR Implants ®) (n = 10) foram subdividas em cinco grupos: controle, tratamento 1, 2, 3 e 4, conforme as reutilizações dos ácidos. As capturas dos implantes no aumento de 500x, 1000x, 2000x e 4000x foram realizadas no microscópio eletrônico de varredura, para posterior análise de rugosidade pelo software ImageJ. Os valores de Ra e Rq foram analisados estatisticamente pelo teste ANOVA e o pós-teste de Tukey. Resultado: Os dados obtidos pelas imagens capturadas e pelos números de Ra e Rq adquiridos pelo ImageJ demonstraram que o tratamento com o duplo ataque ácido com cinco utilizações dos mesmos ácidos foi positivo para o tratamento de superfície do implante de liga de titânio. Conclusão: Pode-se concluir que até quatro reutilizações dos ácidos não interferiu estatisticamente nos valores de rugosidade em diferentes aumentos. São necessários mais estudos referentes à reutilização dos ácidos, contribuindo para a diminuição dos custos aos fabricantes, aumentando a sustentabilidade e mantendo-se a qualidade do produto.


Introduction: The importance of roughness for osseointegration is due to the configuration of proteins with the surface of the implant, and adsorption. Different methods are used in surface treatments, in which parts of the surface layer are removed, such as acid attack. Objective: To analyze changes in roughness on the surface of osseointegrated implants treated by double acid etching with single-use and up to 4 reuses of serums at a magnification of 500x, 1000x, 2000x, and 4000x in the scanning microscope (SEM). Method Samples of adherent implants (SINGULAR Implants ®) of lever alloy (n=10) were subdivided into 5 groups: control, treatment 1, 2, 3, and 4, according to the reuses. For the surface topography of the samples, SEM was used, followed by analysis by ImageJ software. Using the ANOVA test and Turkeys post-test, Ra and Rq values were statistically analyzed. Result: The data obtained both by the images captured in the SEM and by the Ra and Rq numbers acquired by the ImageJ illustrate that the treatment with the double acid attack with 5 uses of the same ones served, was positive for the surface treatment of the alloy implant of independent. Conclusion: It can be concluded that up to four reuses of food do not statistically interfere with roughness values. More studies are needed regarding the reuse of acids, certainly to reduce costs to manufacturers, increasing sustainability while maintaining product quality.


Assuntos
Propriedades de Superfície , Titânio , Implantes Dentários , Análise de Variância , Osseointegração , Adsorção , Microscopia Eletrônica de Varredura
8.
Braz. j. oral sci ; 22: e237545, Jan.-Dec. 2023. tab
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-1433748

RESUMO

Aim: To evaluate dentin permeability after pretreatment with 2.5% aqueous solution of titanium tetrafluoride (TiF4), followed by a self-etching universal adhesive system. Methods: Forty dentin discs (1.5 mm thick) were randomly divided into groups according to the application or non-application of a pretreatment, and the type of adhesive system to be tested (two-step self-etching/ Clearfil SE Bond/ Kuraray Medical, or universal adhesive system/ Single Bond Universal/ 3M ESPE). Both sides of the discs were conditioned with 37% phosphoric acid to remove the smear layer. The first hydraulic conductivity measurement (L1) was performed in a permeability machine, under 5 PSI pressure. The samples were sanded again to form a standardized smear layer. The teeth designated for pre-treatment with TiF4 received the TiF4 solutions applied actively for 60 seconds, and the adhesive systems were applied according to the manufacturer's instructions. Then, a new hydraulic conductivity measurement (L2) was performed for the purpose of calculating the hydraulic conductance at a later time, considering the water viscosity and the thickness of the specimen. The percentage (L) of dentin permeability after application of the adhesive system was obtained (L (%) = [(L1-L2) x100] / L1). The Mann-Whitney non-parametric test was applied. Results: There was no difference between the two adhesive systems, or between the groups with or without pretreatment, as regards dentin permeability (p>0.05). Conclusion: Pretreatment with 2.5% TiF4 did not influence dentin permeability, irrespective of the adhesive system used


Assuntos
Titânio , Adesivos Dentinários , Permeabilidade da Dentina , Fluoretos
9.
Pesqui. bras. odontopediatria clín. integr ; 23: e210155, 2023. tab, graf
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-1507020

RESUMO

ABSTRACT Objective: To evaluate the mechanical properties of mini-implants (MIs) manufactured from stainless steel and compare them with conventional titanium-aluminum-vanadium alloy MIs. Material and Methods: The following groups were formed: G1 (n=24), 8×1.5 mm steel MIs; G2 (n=24), 12×2.0 mm steel MIs; and G3 (n=24), 10×1.5 mm titanium MIs. The 72 MIs were inserted in the infra zygomatic crest region of the maxilla and retromolar trigone in the jaw of 10 pigs. Pull-out, insertion torque, fracture and percussion tests were performed in order to measure the tensile strength, primary stability and fracture strength of MIs. A digital torque gauge was used to measure insertion and fracture torque, a universal mechanical testing machine was used for pull-out testing and a periotest device was used to measure the micromovement of MIs. For morphological and MI component evaluation, scanning electron microscopy (SEM) was performed. D'Agostino & Pearson, Kruskal-Wallis, and Dunn post-hoc and normality tests were used. Results: G2 insertion and fracture torques were significantly higher than G1 and G3 insertion and fracture torques (p<0.05). The pull-out and percussion tests presented similar values among the groups. SEM revealed that the fracture point was predominantly on the fourth thread for steel MIs (G1 and G2) and on the seventh thread for titanium-aluminum-vanadium MIs (G3). Conclusion: The mechanical properties of stainless steel MIs are superior to those of titanium-aluminum-vanadium alloy MIs.


Assuntos
Animais , Aço Inoxidável/química , Resistência à Tração , Titânio , Procedimentos de Ancoragem Ortodôntica/instrumentação , Suínos , Microscopia Eletrônica de Varredura/instrumentação , Estatísticas não Paramétricas , Resistência à Flexão , Testes Mecânicos
10.
Rev. cir. (Impr.) ; 74(3): 263-268, jun. 2022. graf, tab
Artigo em Espanhol | LILACS | ID: biblio-1407920

RESUMO

Resumen Objetivo: Analizar la prevalencia y los factores en la remoción de elementos de osteosíntesis (OTS) de pacientes tratados quirúrgicamente debido a fracturas maxilofaciales. Materiales y Método: Estudio retrospectivo descriptivo, donde fueron incluidos todos los pacientes con diagnóstico de fractura maxilofacial y tratados mediante reducción abierta y fijación interna rígida en un intervalo de 10 años, en el Servicio de Cirugía Oral y Maxilofacial en el Hospital Clínico Mutual de Seguridad (HCMS). Resultados: En un total de 807 pacientes intervenidos, con un rango etario entre 22-66 años, fueron utilizados 2.421 OTS. Entre ellos, 58 pacientes (7,2%) fueron sometidos a un segundo procedimiento quirúrgico, retirándose un total de 129 OTS (5,3%). La principal causa de retiro fue infección (41,1%), comúnmente de carácter tardío. El tercio inferior facial fue el más afectado, específicamente, la zona parasinfisiaria. El 39% fue retirado antes de los 12 meses de posicionados. Conclusiones: El retiro de OTS, posterior a trauma maxilofacial tiene una baja prevalencia. El sitio más afectado es el hueso mandibular y la mayoría se retira dentro de los primeros 12-24 meses. La etiología es variable, sin embargo, la infección se mantiene como una de las principales. Los hallazgos sugieren que no sería recomendable realizar este procedimiento de forma universal para todos los pacientes.


Aim: To analyse the prevalence and factors regarding to osteosynthesis elements (OTS) removal from patients surgically treated due to maxillofacial fractures. Materials and Method: Retrospective study in which all patients with diagnosis of maxillofacial fractures and treated with open reduction and internal rigid fixation were included, in an interval of 10 years, in the Maxillofacial Surgery Service of HCMS. Results: In 807 surgically treated patients, with an age between 22-66 years, 2.421 OTS were used. Among them, 58 patients (7.2%) underwent a second surgical procedure, with a total of 129 OTS removed (5.3%). The main cause of removal was infection (41.1%), commonly of a chronic nature. The lower third of the face was the most affected, specifically, the parasymphysis region. 39% of OTS were withdrawn before 12 months. Conclusions: OTS removal after maxillofacial trauma has a low prevalence, the most affected site is the mandibular bone, within the first 12-24 months. The aetiology is variable, however, infection remains one of the main. The findings suggest that it would not be advisable to perform this procedure universally for all patients.


Assuntos
Humanos , Titânio , Remoção de Dispositivo , Traumatismos Maxilofaciais/cirurgia , Cirurgia Bucal , Fixação Interna de Fraturas
11.
Rev. Fac. Odontol. Univ. Antioq ; 34(1): 14-30, ene.-jun. 2022. tab, graf
Artigo em Inglês | LILACS | ID: biblio-1394659

RESUMO

Abstract Introduction: Nickel-Titanium (NiTi) endodontic files are made of hyperelastic material with shape memory. However, these files suffer a sudden fracture during the endodontic treatment, which is considered an unfavorable prognosis. Many studies have been conducted to establish fatigue resistance focused on file brands and determine which is better. Although the most common failure mechanisms have been established for motorized endodontic files, the information is scattered, making it difficult to develop clear research trends. Methods: a scoping review was carried out using Scopus, Dimensions.ai, Web of Science, and Science Direct databases to answer screening questions related to the predominant fracture mechanism in NiTi files, test types, and equipment used for experimentation and to identify the most active authors. Results: using the general search terms, 432 research papers were found, of which 75 were finally selected after eliminating duplicates and applying exclusion criteria. Conclusions: typical failure mechanisms for rotatory and reciprocating files were identified based on the panoramic review and bibliometric indicators. Also, the standard mechanical tests for endodontic files and the characteristics of their assemblies were summarized. The most active authors in the area and their nationality were tagged. Finally, gaps for future research are proposed to generate a comprehensive knowledge of NiTi file failure.


Resumen Introducción: las limas de Níquel-Titanio (NiTi) utilizadas en endodoncia están hechas de un material hiperelástico con memoria de forma. Sin embargo, estas limas sufren fractura repentina durante el tratamiento, lo cual se considera un pronóstico desfavorable. Se han realizado diversos estudios para establecer la resistencia a la fatiga de limas, y determinar cuál marca es mejor. Aunque se han establecido los mecanismos de falla más comunes para las limas de endodoncia motorizadas, la información se encuentra dispersa, dificultando la definición de tendencias claras de investigación. Métodos: se realizó una revisión de cobertura temática utilizando las bases de datos Scopus, Dimensions.ai, Web of Science y Science Direct, para responder a preguntas orientadoras relacionadas con el mecanismo de fractura predominante en las limas NiTi, tipos de pruebas y equipos utilizados para la experimentación e identificar los autores más activos en el área. Resultados: utilizando términos generales de búsqueda, se encontraron 435 trabajos de investigación. Finalmente se seleccionaron 75, tras eliminar duplicados y aplicar criterios de exclusión. Conclusiones: a partir de la revisión panorámica de literatura y empleando algunos indicadores bibliométricos, se identificaron los mecanismos de falla más comunes para las limas rotatorias y reciprocantes. Se obtuvo información sobre ensayos mecánicos y los montajes más utilizados para las limas de endodoncia. Se identificaron los autores más activos en el área y su nacionalidad. Por último, se sugieren oportunidades de investigación para generar un conocimiento exhaustivo sobre la falla de las limas NiTi.


Assuntos
Titânio , Endodontia , Níquel , Revisão
12.
Rev. bras. anal. clin ; 54(1): 77-81, 20220330. graf
Artigo em Português | LILACS | ID: biblio-1395764

RESUMO

Objetivo: Esse trabalho objetiva identificar e caracterizar o desenvolvimento da bactéria Pseudomonas aeruginosa forte produtora de biofilme nos seguintes materiais ortopédicos: hastes de titânio e de cromo-cobalto. Método: A quantidade de biofilme formada nas amostras foi avaliada com base na quantidade de Pseudomonas aeruginosa, compondo o biofilme das amostras. Resultado: A formação de biofilme nas ligas de titânio foi significativamente maior do que o observado nas ligas cromo-cobalto, tanto no período de 17 horas quanto em uma semana. O cromo-cobalto possibilitou a formação de maior número de biofilme em uma semana, enquanto o titânio viabilizou maior geração de biofilme no período de 17 horas. Além disso, observou-se que um período de maior permanência do biomaterial em contato com a bactéria não pode ser considerado como um fator de proteção no processo de formação de biofilme. Desse modo, evidenciamos a necessidade de investimento em pesquisas relacionadas à prevalência e desenvolvimento de biofilme em ligas metálicas largamente utilizadas nos implantes cirúrgicos. Conclusão: O tempo influenciou apenas na formação de bactéria no cromo-cobalto, sendo quanto maior tempo de contato com a bactéria, maior quantidade de biofilme. Entre as ligas metálicas titânio e cromo-cobalto, o cromo-cobalto produziu menor quantidade de biofilme.


Objective: This work aims to identify and characterize the development of the bacterium Pseudomonas aeruginosa forte that produces biofilm in the following orthopedic materials: titanium and chromium-cobalt rods. Method: The amount of biofilm formed in the samples was evaluated based on the amount of Pseudomonas aeruginosa composing the biofilm of the samples. Result: The biofilm formation in titanium alloys was significantly higher than that observed in chromium-cobalt alloys both in 17 hours and in a week. Chromium-cobalt enabled the formation of a greater number of biofilms in one week, while titanium enabled greater generation of biofilms in 17 hours. In addition, it was observed that a period of greater permanence of the biomaterial in contact with the bacteria cannot be considered as a protective factor in the biofilm formation process. Thus, we highlight the need for investment in research related to the prevalence and development of biofilm in metal alloys widely used in surgical implants. Conclusion: Time influenced only the formation of bacteria in chromium-cobalt, the longer the contact with the bacteria, the greater the amount of biofilm. Among the titanium and chromium-cobalt metal alloys, chromium-cobalt produced less biofilm.


Assuntos
Materiais Biocompatíveis , Biofilmes , Infecções , Pseudomonas aeruginosa , Coluna Vertebral , Titânio , Ligas de Cromo
13.
Int. j. morphol ; 40(1): 188-193, feb. 2022. ilus
Artigo em Inglês | LILACS | ID: biblio-1385596

RESUMO

SUMMARY: The utility of metallic bio-medical implants in osseous or dental affections is irrefutable. The paper aims to test the tolerance of the bone marrow to titanium implants. Titanium implants were inserted in the femur of 11-months old rabbits. The implants penetrated the endosteum, half of their length getting into the haematogenous bone marrow. Seven days after the insertion we collected bone fragments containing the implant. The CT exam revealed a significant decrease in the density of the bone at the interface with the implant and a more discrete one aloof from the insertion area. The histologic exam after 7 days revealed osseous reparatory processes only in the endosteal area from where it expanded on the surface of the implant which was inside the marrow. The presence and intensity of the osseous reparatory processes after only seven days post-implant demonstrates that the marrow actively participates in bone regeneration and implants osseointegration.


RESUMEN: La utilidad de los implantes biomédicos metálicos en afecciones óseas o dentales es irrefutable. El documento tiene como objetivo probar la tolerancia de la médula ósea a los implantes de titanio. Se insertaron implantes de titanio en el fémur de conejos de 11 meses. Los implantes penetraron en el endostio y la mitad de su longitud penetró en la médula ósea hematógena. Siete días después de la inserción, recolectamos fragmentos de hueso que contenían el implante. El examen de TC reveló una disminución significativa en la densidad del hueso en la interfaz con el implante y una más discreta alejada del área de inserción. El examen histológico a los 7 días reveló procesos de reparación ósea solo en el área endóstica desde donde se expandió en la superficie del implante que estaba dentro de la médula. La presencia e intensidad de los procesos de reparación ósea después de solo siete días del implante demuestra que la médula ósea participa activamente en la regeneración ósea y en la osteointegración de los implantes.


Assuntos
Humanos , Próteses e Implantes , Titânio/química , Medula Óssea , Osseointegração/fisiologia , Regeneração Óssea/fisiologia
14.
Cienc. tecnol. salud ; 9(1): 82-97, 2022. il^c27
Artigo em Inglês | LILACS, DIGIUSAC, LIGCSA | ID: biblio-1390741

RESUMO

White cement-based mortars in urban areas are usually discolored and altered their esthetic properties due to air pollutants. The addition of nanoparticles in these mortars can provide photocatalytic properties that can decompose pollution agents. Likewise, other hydrophobic agents have been individually studied to improve outdoor building constructions. Therefore, this study presented the photocatalytic and hydrophobic effect of adding nano-TiO2and silicone hydrophobic powder (DOWSILTM) in a white cement matrix. The nano-TiO2 were characterized by X-Ray Diffraction (XRD); afterwards, the mortar was mixed with additions of nano-TiO2 (0.0, 0.5, 1.0, 3.0%) and DOWSILTM (0.0, 0.5%). The mortar's photocatalytic performance was evaluated using a modification of the standard Italian test Ente Nazionale Italiano di Unificazione 11259:2016 based on Rhodamine B (RhB) degradation on the sample exposed to UV irradiation. Therefore, mortar samples were subjected to UV irradiation to degrade the organic dye rhodamine B, monitoring their color variation using a C I E L* a* b* spectrophotometer. Moreover, the water permeability and the contact angle were evaluated. This research demonstrates that the white cement-based mortar samples added with nano-TiO2/DOWSILTM possess photocatalytic activity. The samples with the addition of 1.0%/0.5% and 3.0%/0.5% nano-TiO2/DOWSILTM showed a higher RhB degradation for R4 and R26. Therefore, these two materials can be employed in these proportions to improve the quality of the white cement-based mortars in urban constructions.


Los morteros a base de cemento blanco generalmente se decoloran y alteran sus propiedades estéticas debido a los contaminantes del aire en las áreas urbanas. Nanopartículas añadidas a estos morteros pueden proporcionar propiedades fotocatalíticas que descomponen estos contaminantes. Asimismo, otros agentes hidrofóbicos se han estu-diado individualmente para mejorar las construcciones a la intemperie. Por lo tanto, se presenta el efecto fotocatalítico e hidrofóbico al incorporar nano-TiO2 y silicona hidrofóbica de polisiloxano (DOWSILTM) en una matriz de cemento blanco. El nano-TiO2 se caracterizó por medio de Difracción de Rayos X (DRX); luego, el mortero se mezcló con adiciones de nano-TiO2 (0.0, 0.5, 1.0, 3.0%) y DOWSILTM (0.0, 0.5%). Los morteros se sometieron a irradiación UV, para degradar el colorante orgánico rodamina B, monitoreando su variación de color usando un espectrofotómetro C I E L* a* b*. La eficiencia fotocatalítica del mortero se evaluó utilizando una modificación de la norma italiana Ente Nazionale Italiano di Unificazione 11259:2016 basada en la degradación de la rodamina B (RhB) en el mortero expuesto a la radiación UV. Además, se evaluó la permeabilidad al agua y el ángulo de contacto. Esta investigación demostró que el mortero de cemento con nano-TiO2/ DOWSILTM posee actividad fotocatalítica. Las muestras con 1.0%/0.5% y 3.0%/0.5% nano-TiO2/DOWSILTM mostraron una mayor eficiencia de degradación de RhB para R4 y R26. Por lo tanto, estos materiales tienen potencial para mejorar la calidad de los morteros en construcciones urbanas.


Assuntos
Poluentes Atmosféricos , Absorção , Nanopartículas , Permeabilidade , Silicones/análise , Titânio/análise , Materiais de Construção/análise
15.
Artigo em Espanhol | LILACS, BINACIS | ID: biblio-1367132

RESUMO

Introducción: Se dispone de una amplia variedad de opciones terapéuticas para la reconstrucción de defectos óseos segmentarios causados por fracturas, tumores o infecciones, pero aún es un desafío en la cirugía ortopédica. materiales y métodos:Se presentan seis casos de pacientes con pérdida ósea masiva tratados mediante lo que denominamos "combinación sinérgica" de una membrana inducida para aportar beneficios biológicos, más un andamiaje (scaffold) de titanio trabecular desarrollado especialmente, según cada paciente, para el aporte de estabilidad y estructura. Resultados: Cinco hombres y una mujer (edad promedio 30 años) fueron operados con esta técnica. El seguimiento promedio fue de 24 meses. En el posoperatorio inmediato, se logró el restablecimiento del eje, la longitud y la estabilidad mecánica suficiente para iniciar la carga parcial. La carga total, según las condiciones del paciente (dolor, fuerza muscular), demandó un promedio de 25 a 30 días. Conclusiones: Proponemos una opción de tratamiento poco frecuente en nuestro medio que brinda estabilidad biomecánica suficiente para tolerar la carga precoz recuperando la longitud total del defecto en un solo acto, con excelentes resultados funcionales, entendiendo estas como ventajas frente a las opciones terapéuticas de uso tradicional, como transporte o técnica de Masquelet. Nivel de Evidencia: IV


Introduction: There is a wide variety of therapeutic options for the reconstruction of segmental bone defects caused by fractures, tumors, or infections, but it continues to be a challenge in orthopedic surgery. materials and methods: The present work presents six (6) cases of patients with massive bone loss treated by means of what we call a "synergistic combina-tion" of an induced membrane, to provide biological benefits, plus a trabecular titanium scaffold designed for each patient to provide stability and structure. Results: Five men and one woman with an average age of 30 years were operated on by this technique. The average follow-up was 24 months. In the immediate postoperative period, the axis, length, and sufficient mechanical stability to initiate partial weight-bearing were reestablished. Full weight-bearing according to the patients' conditions (pain, muscle strength) required an average of 25 to 30 days. Conclusion: We propose a rare treatment option in our field with sufficient biomechanical stability to tolerate early weight-bearing, recovering the entire length of the defect in a single stage with excellent functional outcomes, understanding these as an advantage over traditional therapeutic options such as bone transport or the Masquelet technique. Level of Evidence: IV


Assuntos
Próteses e Implantes , Titânio , Osso e Ossos , Transplante Ósseo , Procedimentos de Cirurgia Plástica
16.
Braz. j. biol ; 82: e237214, 2022. tab, graf
Artigo em Inglês | LILACS, VETINDEX | ID: biblio-1249258

RESUMO

Artemisia absinthium L. is an important herb that is widely cultivated in different parts of the world for its medicinal properties. The present study evaluated the effects of four concentrations of nanoparticles treatment (0, 10, 20 and 30 mg L-1) and NaCl salinity stress (0, 50, 100 and 150 mM NaCl) and their interactions with respect to the expression of two key genes, i.e. DBR2 and ADS, in the biosynthesis pathway of artemisinin in A. absinthium. Total RNA was extracted and a relative gene expression analysis was carried out using Real-Time PCR. The amount of artemisinin was also determined by HPLC. All the experiments were performed as factorial in a completely randomized design in three replications. The results revealed that salinity stress and nanoparticles treatment and their interaction affected the expressions of these genes significantly. The highest levels of ADS gene expression were observed in the 30 mg L-1 nanoparticles­treated plants in the presence of 150 mM salinity stress and the lowest levels in the 10 mg L-1 nanoparticles­treated plants under 50 mM salinity stress. The maximum DBR2 gene expression was recorded in the 10 mg L-1 nanoparticles­treated plants in the absence of salinity stress and the minimum expression in the 100 mM salinity-stressed plants in the absence of nanoparticles treatment. Moreover, the smallest amounts of artemisinin were observed in the 150 mM salinity-stressed plants in the absence of nanoparticles and the highest amounts in the 30 mg L-1 nanoparticles­treated plants. The maximum amounts of artemisinin and ADS gene expression were reported from the plants in the same nanoparticles treatment and salinity stress conditions. In this regard, the amount of artemisinin was decreased by half in the plants containing the highest DBR2 gene expression. Meanwhile, no significant correlation was observed between these gene expressions and the artemisinin amount in the other nanoparticles­treated plants under different levels of salinity stress. The biosynthetic pathway of secondary metabolites appears to be very complex and dose not directly dependent on these gene expressions.


Artemisia absinthium L. é uma erva importante que é amplamente cultivada em diferentes partes do mundo por suas propriedades medicinais. O presente estudo avaliou os efeitos de quatro concentrações de tratamento com nanopartículas (0, 10, 20 e 30 mg L-1) e estresse de salinidade com NaCl (0, 50, 100 e 150 mM NaCl) e suas interações com relação à expressão de dois genes-chave, isto é, DBR2 e ADS, na via de biossíntese da artemisinina em A. absinthium. O RNA total foi extraído, e uma análise de expressão gênica relativa foi realizada usando PCR em tempo real. A quantidade de artemisinina também foi determinada por HPLC. Todos os experimentos foram realizados como fatorial, em delineamento inteiramente casualizado, em três repetições. Os resultados revelaram que o estresse por salinidade e o tratamento com nanopartículas e sua interação afetaram significativamente as expressões desses genes. Os níveis mais altos de expressão do gene ADS foram observados nas plantas tratadas com nanopartículas de 30 mg L-1 na presença de estresse de salinidade de 150 mM, e os níveis mais baixos, nas plantas tratadas com nanopartículas de 10 mg L-1 com estresse de salinidade de 50 mM. A expressão máxima do gene DBR2 foi registrada nas plantas tratadas com nanopartículas de 10 mg L-1 na ausência de estresse de salinidade, e a expressão mínima, nas plantas estressadas com salinidade de 100 mM na ausência de tratamento com nanopartículas. Além disso, as menores quantidades de artemisinina foram observadas nas plantas com estresse de salinidade de 150 mM na ausência de nanopartículas, e as maiores quantidades, nas plantas tratadas com nanopartículas de 30 mg L-1. As quantidades máximas de expressão de genes de artemisinina e ADS foram relatadas a partir das plantas no mesmo tratamento com nanopartículas e condições de estresse de salinidade. A esse respeito, a quantidade de artemisinina diminuiu pela metade nas plantas que contêm a expressão gênica DBR2 mais alta. Enquanto isso, nenhuma correlação significativa foi observada entre essas expressões gênicas e a quantidade de artemisinina nas outras plantas tratadas com nanopartículas sob diferentes níveis de estresse de salinidade. A via biossintética dos metabólitos secundários parece ser muito complexa e não depende diretamente dessas expressões gênicas.


Assuntos
Artemisia absinthium/genética , Artemisia annua , Artemisininas , Nanopartículas , Proteínas de Plantas , Titânio , Estresse Salino
17.
Pesqui. bras. odontopediatria clín. integr ; 22: e210120, 2022. tab, graf
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-1422283

RESUMO

Abstract Objective: To examine the cyclic fatigue resistance and surface topography of TruNatomy and ProTaper Gold nickel-titanium rotary files and evaluate the presence of alterations to surface topography following instrumentation in simulated curved canals. Material and Methods: Twenty-four nickel-titanium instruments, twelve each of TN and PTG file systems, were evaluated for cyclic fatigue resistance. The rotary files were rotated in a simulated root canal with standardized diameter, angle of curvature, and radius of curvature in a custom-made cyclic fatigue testing device until the instrument fracture occurred. The time to fracture for each instrument was recorded with a stopwatch; in seconds in each group. Fractured instruments were subjected to atomic force microscopy analysis measuring the average roughness and the root mean square values to investigate surface features of endodontic files. Mean values and standard deviation were calculated. Data were analyzed using the Mann-Whitney U test. Results: Time to fracture was marginally higher in PTG instruments than in the TN file systems. PTG files exhibited higher surface roughness when compared with TN files (p<0.05). Conclusion: TN file system had a higher cyclic fatigue resistance than PTG. Cyclic fatigue causing file breakage did affect the surface topography of the files. PTG files showed a higher surface porosity value than the TN files (AU).


Assuntos
Titânio/química , Microscopia de Força Atômica/instrumentação , Ligas Dentárias , Instrumentos Odontológicos , Endodontia , Propriedades de Superfície , Estatísticas não Paramétricas , Cavidade Pulpar , Testes de Dureza , Níquel/química
18.
Rev. odontol. UNESP (Online) ; 51: e20220046, 2022. tab, ilus
Artigo em Português | LILACS, BBO - Odontologia | ID: biblio-1424236

RESUMO

Introdução: É importante saber se o hipoclorito de sódio (NaOCl) influencia a resistência à fadiga cíclica das limas de níquel-titânio (NiTi). Objetivo: Avaliar a influência de NaOCl 2,5% na resistência à fadiga cíclica de dois sistemas de NiTi. Material e método: 40 instrumentos rotatórios - 20 TruNatomy® (TRU, Dentsply Sirona, Maillefer, Ballaigues, Suíça) e 20 Prodesing Logic2® (PDL2, Bassi, Belo Horizonte, Minas Gerais, Brasil) - foram aleatoriamente distribuídos em 4 grupos experimentais (n = 10) imersos em água destilada (H2O) e NaOCl 2,5% em temperatura a 37°C. Foram submetidos a testes de fadiga cíclica mensurando o número de ciclos para fratura (NCF) e análise dessas superfícies pós-teste em microscópio eletrônico por varredura. Para a análise estatística entre os grupos, foi aplicada a análise de variância (ANOVA), complementada com o pós-teste de Tukey. Resultado: Houve diferença estatística em todos os grupos (P<0.05). Os instrumentos PDL2 obtiveram maior resistência à fratura nas condições em H2O e em NaOCl 2,5% comparados aos instrumentos TRU. Na análise de grupos de instrumentos nas soluções de NaOCl e H2O, foi observado que o NaOCl 2,5% diminuiu o NCF. Conclusão: A resistência à fadiga cíclica dos instrumentos TRU e PDL2 diminuiu com NaOCl 2,5%. Os instrumentos PDL2 foram mais resistentes à fratura em relação aos instrumentos TRU.


Introduction: It is important to know whether sodium hypochlorite (NaOCl) influences the cyclic fatigue resistance of nickel-titanium (NiTi) files. Objective: To evaluate the influence of NaOCl 2.5% on the cyclic fatigue resistance of two NiTi systems. Material and method: Forty rotary instruments - 20 TruNatomy® (TRU, Dentsply Sirona, Maillefer, Ballaigues, Switzerland) and 20 Prodesign Logic2® (PDL2, Bassi, Belo Horizonte, Minas Gerais, Brazil) - were distributed randomly across four experimental groups (n=10) and submerged in distilled water (H2O) or 2.5% NaOCl at 37°C according to allocation. Cyclic fatigue testing was then performed, measuring the number of cycles to fracture (NCF), and post-test surfaces were analysed by scanning electron microscopy (SEM). Statistical Analysis: Analysis of variance (ANOVA) was applied for between-group analysis, followed by Tukey's post-hoc test. Result: A significant difference was observed in all groups (P<0.05). PDL2 instruments showed higher fracture resistance under H2O and 2.5% NaOCl conditions compared to TRU. Analysis of all instrument groups showed that exposure to 2.5% NaOCl decreased the NCF compared to H2O. Conclusion: Cyclic fatigue resistance of the TRU and PDL2 instruments was decreased by exposure to 2.5% NaOCl. PDL2 instruments were more resistant to fracture than TRU instruments.


Assuntos
Hipoclorito de Sódio , Titânio , Microscopia Eletrônica de Varredura , Análise de Variância , Instrumentos Odontológicos , Níquel , Tratamento Térmico , Corrosão
19.
Braz. dent. sci ; 25(1): 1-9, 2022. ilus
Artigo em Inglês | LILACS, BBO - Odontologia | ID: biblio-1353788

RESUMO

Objective: The objective of this study was to evaluate in vitro the influence of the anodized surface of Ti35Nb7Zr alloy on the behavior of osteogenic cells, for future application in biomedical implants. Material and Methods: For the development of this research, samples of commercially pure titanium (TiCp) and samples of Ti35Nb7Zr alloy were anodized, both were characterized by scanning electron microscopy (SEM) and were plated afterwards with human osteoblast-like cells (MG63 line) (2 x 104). Cell adhesion, cytotoxicity test, formation of mineralization nodules and a comet assay were also performed in different periods. The bottom of the plate was used as a control, without a sample. Results: SEM analysis showed that the topography of both samples presented surfaces covered by nanotubes. Cellular morphology exhibited spreading in both samples proposing an intimate cell- material liaison. After 3 days, the Ti35Nb7Zr group exhibited greater cell viability than the TiCp group (p<0.01). Regarding calcium content, there was no statistical difference between the anodized groups, but there was a difference between the experimental groups and the control group (p<0.01). In the comet assay, the percentage of DNA in the comet tail did not exhibit any significant difference (p>0.05) among the groups in the evaluated periods. Conclusion: It was concluded that this process of anodization was efficient to form nanotubes, as well as promote a positive influence on the behavior of osteogenic cells without promoting cell damage. (AU)


Objetivo: O objetivo deste estudo foi avaliar in vitro a influência da superfície anodizada da liga Ti35Nb7Zr no comportamento de células osteogênicas, para futura aplicação em implantes biomédicos. Material e Métodos: Para o desenvolvimento desta pesquisa, amostras de titânio comercialmente puro (TiCp) e amostras da liga Ti35Nb7Zr foram anodizadas, ambas foram caracterizadas por microscopia eletrônica de varredura (MEV) e posteriormente plaqueadas com células semelhantes a osteoblastos humanos (linha MG63) (2 x 104). Foram realizados em diferentes períodos a adesão celular, teste de citotoxicidade, formação de nódulos de mineralização e ensaio do cometa. O fundo da placa foi usado como controle, sem amostra. Resultados: A análise em MEV mostrou que a topografia de ambas as amostras apresentava superfícies cobertas por nanotubos. A morfologia celular exibiu espalhamento em ambas as amostras, propondo uma ligação íntima célula-material. Após 3 dias, o grupo Ti35Nb7Zr exibiu maior viabilidade celular do que o grupo TiCp (p<0.01). Em relação ao teor de cálcio, não houve diferença estatística entre os grupos anodizados, mas houve diferença entre os grupos experimentais e o grupo controle (p<0.01). No ensaio do cometa, a porcentagem de DNA na cauda do cometa não apresentou diferença significativa (p> 0.05) entre os grupos nos períodos avaliados. Conclusão:Concluiu-se que esse processo de anodização foi eficiente para formar nanotubos, além de promover uma influência positiva no comportamento das células osteogênicas sem promover dano celular. (AU)


Assuntos
Osteoblastos , Titânio
20.
Rev. bras. oftalmol ; 81: e0008, 2022. graf
Artigo em Inglês | LILACS | ID: biblio-1360919

RESUMO

ABSTRACT Minimally invasive glaucoma surgeries are surgical treatment alternatives for glaucoma aimed at reducing intraocular pressure with a better safety profile compared to traditional trabeculectomy. However, in spite of less invasive techniques, complications may develop in any surgical procedure. To the best of our knowledge, this is the first case report of anterior uveitis following combined treatment with cataract surgery and iStent inject® which addresses the management of postoperative inflammation.


RESUMO As cirurgias minimamente invasivas para glaucoma consistem em uma opção de tratamento cirúrgico para glaucoma, a qual promove redução da pressão intraocular com melhor perfil de segurança do que a trabeculectomia. Todavia, complicações são inerentes à realização de procedimentos cirúrgicos, apesar do uso de técnicas menos invasivas. Este é o primeiro relato que apresenta um caso de uveíte anterior após cirurgia combinada de catarata e iStent inject®, além de orientações quanto ao manejo do quadro inflamatório.


Assuntos
Humanos , Feminino , Pessoa de Meia-Idade , Uveíte/tratamento farmacológico , Extração de Catarata/efeitos adversos , Uveíte Anterior/etiologia , Complicações Pós-Operatórias , Titânio , Malha Trabecular/cirurgia , Tropicamida/administração & dosagem , Dexametasona/administração & dosagem , Stents , Glaucoma de Ângulo Aberto/cirurgia , Injeções Intraoculares , Pressão Intraocular , Acetazolamida/administração & dosagem