In vitro chipping behaviour of all-ceramic crowns with a zirconia framework and feldspathic veneering: comparison of CAD/CAM-produced veneer with manually layered veneer.
Schmitter, M; Mueller, D; Rues, S.
Afiliación
  • Schmitter M; Section for Biomaterial Research, Department of Prosthodontics, University of Heidelberg, Heidelberg, Germany.
J Oral Rehabil ; 40(7): 519-25, 2013 Jul.
Article en En | MEDLINE | ID: mdl-23663118
ABSTRACT
The purpose of this in vitro study was to assess the breaking load of zirconia-based crowns veneered with either CAD/CAM-produced or manually layered feldspathic ceramic. Thirty-two identical zirconia frameworks (Sirona inCoris ZI, mono L F1), 0·6 mm thick with an anatomically shaped occlusal area, were constructed (Sirona inLab 3.80). Sixteen of the crowns were then veneered by the use of CAD/CAM-fabricated feldspathic ceramic (CEREC Bloc, Sirona) and 16 by the use of hand-layered ceramic. The CAD/CAM-manufactured veneer was attached to the frameworks by the use of Panavia 2.0 (Kuraray). Half of the specimens were loaded until failure without artificial ageing; the other half of the specimens underwent thermal cycling and cyclic loading (1·2 million chewing cycles, force magnitude F(max) = 108 N) before the assessment of the ultimate load. To investigate the new technique further, finite element (FE) computations were conducted on the basis of the original geometry. Statistical assessment was made by the use of non-parametric tests. Initial breaking load was significantly higher in the hand-layered group than in the CAD/CAM group (mean 1165·86 N versus 395·45 N). During chewing simulation, however, 87·5% (7/8) of the crowns in the hand-layered group failed, whereas no crown in the CAD/CAM group failed. The CAD/CAM-produced veneer was significantly less sensitive to ageing than the hand-layered veneer.
Asunto(s)

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Asunto principal: Diseño de Prótesis Dental / Fracaso de la Restauración Dental / Coronas / Materiales Dentales / Coronas con Frente Estético Límite: Humans Idioma: En Revista: J Oral Rehabil Año: 2013 Tipo del documento: Article País de afiliación: Alemania

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Asunto principal: Diseño de Prótesis Dental / Fracaso de la Restauración Dental / Coronas / Materiales Dentales / Coronas con Frente Estético Límite: Humans Idioma: En Revista: J Oral Rehabil Año: 2013 Tipo del documento: Article País de afiliación: Alemania
...