Simple Co-Precipitation of Iron Minerals for the Removal of Phenylarsonic Acid: Insights into the Adsorption Performance and Mechanism.
Wang, Lili; Hu, Changchao; Yang, Ze; Guo, Songding; Zhang, Tingting; Li, Shangyi.
Afiliación
  • Wang L; Petroleum Exploration and Production Research Institute, SINOPEC, Beijing 100083, China.
  • Hu C; Petroleum Exploration and Production Research Institute, SINOPEC, Beijing 100083, China.
  • Yang Z; Department of Environmental Science and Engineering, Research Centre for Resource and Environment, Beijing University of Chemical Technology, Beijing 100029, China.
  • Guo S; Department of Environmental Science and Engineering, Research Centre for Resource and Environment, Beijing University of Chemical Technology, Beijing 100029, China.
  • Zhang T; Department of Environmental Science and Engineering, Research Centre for Resource and Environment, Beijing University of Chemical Technology, Beijing 100029, China.
  • Li S; Department of Environmental Science and Engineering, Research Centre for Resource and Environment, Beijing University of Chemical Technology, Beijing 100029, China.
Molecules ; 28(8)2023 Apr 13.
Article en En | MEDLINE | ID: mdl-37110683
In this study, three kinds of iron minerals, ferrihydrite, hematite, and goethite, were prepared by a simple coprecipitation method for the adsorption and removal of phenylarsonic acid (PAA). The adsorption of PAA was explored, and the influences of ambient temperature, pH, and co-existing anions on adsorption were evaluated. The experimental results show that rapid adsorption of PAA occurs within 180 min in the presence of iron minerals, and the adsorption process conforms to a pseudo-second-order kinetic model. The isothermal adsorption of PAA by ferrihydrite, goethite, and hematite agrees with the Redlich-Peterson model. The maximum adsorption capacities of PAA are 63.44 mg/g, 19.03 mg/g, and 26.27 mg/g for ferrihydrite, goethite, and hematite, respectively. Environmental factor experiments illustrated that an alkaline environment will significantly inhibit the adsorption of PAA by iron minerals. CO32-, SiO32-, and PO43- in the environment will also significantly reduce the adsorption performance of the three iron minerals. The adsorption mechanism was analyzed by FTIR and XPS, which indicated that ligand exchange between the surface hydroxyl group and the arsine group leads to the formation of an Fe-O-As bond, and electrostatic attraction between the iron minerals and PAA played an important role in the adsorption.