Your browser doesn't support javascript.
loading
Drying-Time Study in Graphene Oxide.
Tene, Talia; Guevara, Marco; Valarezo, Andrea; Salguero, Orlando; Arias Arias, Fabian; Arias, Melvin; Scarcello, Andrea; Caputi, Lorenzo S; Vacacela Gomez, Cristian.
Afiliação
  • Tene T; Grupo de Fisicoquímica de Materiales, Universidad Técnica Particular de Loja, Loja EC-110160, Ecuador.
  • Guevara M; CompNano, School of Physical Sciences and Nanotechnology, Yachay Tech University, Urcuquí EC-100119, Ecuador.
  • Valarezo A; UNICARIBE Research Center, University of Calabria, I-87036 Rende, Italy.
  • Salguero O; UNICARIBE Research Center, University of Calabria, I-87036 Rende, Italy.
  • Arias Arias F; Facultad de Ciencias, Escuela Superior Politécnica de Chimborazo, Riobamba EC-060155, Ecuador.
  • Arias M; UNICARIBE Research Center, University of Calabria, I-87036 Rende, Italy.
  • Scarcello A; Laboratorio de Nanotecnología, Area de Ciencias Básicas y Ambientales, Instituto Tecnológico de Santo Do-mingo, Av. Los Próceres, Santo Domingo 10602, Dominican Republic.
  • Caputi LS; UNICARIBE Research Center, University of Calabria, I-87036 Rende, Italy.
  • Vacacela Gomez C; Surface Nanoscience Group, Department of Physics, University of Calabria, Via P. Bucci, Cubo 33C, I-87036 Rende, Italy.
Nanomaterials (Basel) ; 11(4)2021 Apr 19.
Article em En | MEDLINE | ID: mdl-33921582
ABSTRACT
Graphene oxide (GO) exhibits different properties from those found in free-standing graphene, which mainly depend on the type of defects induced by the preparation method and post-processing. Although defects in graphene oxide are widely studied, we report the effect of drying time in GO and how this modifies the presence or absence of edge-, basal-, and sp3-type defects. The effect of drying time is evaluated by Raman spectroscopy, UV-visible spectroscopy, and transmission electron microscopy (TEM). The traditional D, G, and 2D peaks are observed together with other less intense peaks called the D', D*, D**, D+G, and G+D. Remarkably, the D* peak is activated/deactivated as a direct consequence of drying time. Furthermore, the broad region of the 2D peak is discussed as a function of its deconvoluted 2D1A, 2D2A, and D+G bands. The main peak in UV-visible absorption spectra undergoes a redshift as drying time increases. Finally, TEM measurements demonstrate the stacking of exfoliated GO sheets as the intercalated (water) molecules are removed.