Sci Rep ; 13(1): 16672, 2023 Oct 04.
Artigo em Inglês | MEDLINE | ID: mdl-37794231

RESUMO

This research aims to fabricate an AlSi10Mg parts using Laser Powder Bed Fusion technique with enhanced structural integrity. The prime novelty of this research work is eliminating the balling and sparring effects, keyhole and cavity formation by attaining effective melt pool formation. Modelling of the Laser Powder Bed Fusion process parameters such as Laser power, scanning speed, layer thickness and hatch spacing is carried out through Complex Proportional Assessment technique to optimize the parts' surface attributes and to overcome the defects based on the output responses such as surface roughness on scanning and building side, hardness and porosity. The laser power of 350 W, layer thickness of 30 µm, scan speed of 1133 mm/s, and hatch spacing of 0.1 mm produces significantly desirable results to achieve maximum hardness and minimum surface roughness and holding the porosity of < 1%. The obtained optimal setting from this research improves the structural integrity of the printed AlSi10Mg parts.

SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA