1.
J Dent ; 37(12): 923-31, 2009 Dec.
Artigo em Inglês | MEDLINE | ID: mdl-19660517

RESUMO

OBJECTIVES: This study examined the effect of saliva contamination on the microtensile bond strength (microTBS) of resin luting cements to dentin. METHODS: For RelyX ARC (ARC, 3M ESPE), dentin surfaces were etched with 32% phosphoric acid. The subgroups were: ARC-control (uncontaminated), ARC-I (saliva contamination, blot-dried), ARC-II (saliva contamination, rinse, blot-dried) and ARC-III (saliva contamination, rinse, re-etch, rinse, blot-dried). For Panavia F 2.0 (PF, Kuraray), the subgroups were: PF-control (uncontaminated), PF-I (saliva contamination, dried), PF-II (saliva contamination, rinse, dried), PF-III (primer, saliva contamination, dried), PF-IV (primer, saliva contamination, dried, primer re-applied) and PF-V (primer, saliva contamination, rinse, dried, primer re-applied). Composite blocks were luted onto dentin using the two cements. Bonded specimens were sectioned into 0.9 mm x 0.9 mm beams for muTBS testing. Representative fractured beams were prepared for fractographic analysis. RESULTS: For ARC, salivary contamination of etched dentin (ARC-I) significantly lowered bond strength (p=0.001). Rinsing saliva off with water (ARC-II) restored bond strength to control level. Re-etching dentin surface after rinsing (ARC-III) resulted in the lowest bond strength (p<0.001). For PF, salivary contamination of dentin before (PF-I) and after application of primer (PF-III and PF-IV) significantly lowered bond strength (p<0.001). Rinsing saliva off with water and re-application of primer (PF-II and PF-V) improved bond strength. CONCLUSION: Saliva contamination during luting deteriorated the bond quality of resin cements. Decontamination by rinsing with water was most effective in restoring the bond strength of RelyX ARC. Decontamination by water-rinsing and primer re-application after rinsing improved the bond strength of Panavia F 2.0.


Assuntos
Colagem Dentária , Dentina/ultraestrutura , Cimentos de Resina/química , Saliva/fisiologia , Condicionamento Ácido do Dente/métodos , Adesividade , Bis-Fenol A-Glicidil Metacrilato/química , Compostos Inorgânicos de Carbono/química , Cimentos Dentários/química , Análise do Estresse Dentário , Adesivos Dentinários/química , Humanos , Teste de Materiais , Metacrilatos/química , Ácidos Fosfóricos/química , Polietilenoglicóis/química , Ácidos Polimetacrílicos/química , Poliuretanos/química , Compostos de Silício/química , Estresse Mecânico , Propriedades de Superfície , Resistência à Tração , Água/química
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA