Egg white protein (EW) is used as surface-active ingredient in aerated food and hydroxypropylmethylcellulose (HPMC) is a polysaccharide that behaves as a surfactant. This study aimed at investigating the effects of process parameters biopolymer concentration (2.0-5.0%, w/w), EW:HPMC ratio (2:1-18:1), pH (3.0-6.0), and the influence of biopolymers' behavior in aqueous solution at different pH on the foaming properties (overrun, drainage, and bubble growth rate). Process parameters had effect on foaming properties. The pH was the major factor influencing the type of EW/HPMC interaction and affected the foaming properties of biopolymer mixture. At pH 3.0, EW and HPMC showed thermodynamic compatibility leading to better foaming properties, higher foaming capacity, and stability than without HPMC addition whereas at pH 4.5 and 6.0, EW and HPMC are incompatible that causes lower stability concerning the disproportionation comparing to foam without HPMC. At pH between 3.0 and 4.5, HPMC improves foaming properties of aerated products.


Assuntos
Antiespumantes/química , Proteínas do Ovo/química , Derivados da Hipromelose/química , Tensoativos/química , Concentração de Íons de Hidrogênio , Água/química
2.
Carbohydr Polym ; 103: 55-61, 2014 Mar 15.
Artigo em Inglês | MEDLINE | ID: mdl-24528700

RESUMO

This study aimed at evaluating the effect of three independent variables: biopolymer concentration (egg white proteins and pectin) (2.0-4.0%, w/w); protein:pectin ratio (15:1-55:1); and temperature (70-80 °C), at pH 3.0, using a central composite design on the foaming properties (overrun, drainage and bubble growth rate). Foams produced with protein:pectin ratio 15:1 showed the lowest bubble growth rate and the greatest drainage, whereas protein:pectin ratio 55:1 presented the lowest drainage. Complexes obtained with protein:pectin ratio 15:1 were close to electroneutrality and showed larger size (95.91 ± 8.19 µm) than those obtained with protein:pectin ratio 55:1 (45.92 ± 3.47 µm) not electrically neutral. Larger particles seemed to build an interfacial viscoelastic network at the air-water interface with reduced gas permeability, leading to greater stability concerning the disproportionation. Soluble complexes of smaller sizes increased viscosity leading to a low drainage of liquid and inhibiting the bubbles coalescence.


Assuntos
Biopolímeros/química , Proteínas do Ovo/química , Pectinas/química , Eletricidade Estática
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA