1.
Angew Chem Int Ed Engl ; : e202412006, 2024 Aug 28.
Artigo em Inglês | MEDLINE | ID: mdl-39193808

RESUMO

Designing solid electrolyte is deemed as an effective approach to suppress the side reaction of zinc anode and active material dissolution of cathodes in liquid electrolytes for zinc metal batteries (ZMBs). Herein, kaolin is comprehensively investigated as raw material to prepare solid electrolyte (KL-Zn) for ZMBs. As demonstrated, KL-Zn electrolyte is an excellent electronic insulator and zinc ionic conductor, which presents wide voltage window of 2.73 V, high ionic conductivity of 5.08 mS cm-1, and high Zn2+ transference number of 0.79. For the Zn//Zn cells, superior cyclic stability lasting for 2200 h can be achieved at 0.2 mA cm-2. For the Zn//NH4V4O10 batteries, stable capacity of 245.8 mAh g-1 can be maintained at 0.2 A g-1 after 200 cycles along with high retention ratio of 81%, manifesting KL-Zn electrolyte contributes to stabilize the crystal structure of NH4V4O10 cathode. These satisfying performances can be attributed to the enlarged interlayer spacing, zinc (de)solvation-free mechanism and fast diffusion kinetics of KL-Zn electrolyte, availably guaranteeing uniform zinc deposition for zinc anode and reversible zinc (de)intercalation for NH4V4O10 cathode. Additionally, this work also verifies the application possibility of KL-Zn electrolyte for Zn//MnO2 batteries and Zn//I2 batteries, suggesting the universality of mineral-based solid electrolyte.

2.
Angew Chem Int Ed Engl ; 62(5): e202215324, 2023 Jan 26.
Artigo em Inglês | MEDLINE | ID: mdl-36446732

RESUMO

The rampant dendrites and hydrogen evolution reaction (HER) resulting from the turbulent interfacial evolution at the anode/electrolyte are the main culprits of short lifespan and low Coulombic efficiency of Zn metal batteries. In this work, a versatile protective coating with excellent zincophilic and amphoteric features is constructed on the surface of Zn metal (ZP@Zn) as dendrite-free anodes. This kind of protective coating possesses the advantages of reversible proton storage and rapid desolvation kinetics, thereby mitigating the HER and facilitating homogeneous nucleation concomitantly. Furthermore, the space charge polarization effect promotes charge redistribution to achieve uniform Zn deposition. Accordingly, the ZP@Zn symmetric cell manifests excellent reversibility at an ultrahigh cumulative plating capacity of 4700 mAh cm-2 and stable cycling at 80 % depth of discharge (DOD). The ZP@Zn//V6 O13 pouch cell also reveals superior cycling stability with a high capacity of 326.6 mAh g-1 .

3.
Chem Sci ; 13(39): 11656-11665, 2022 Oct 12.
Artigo em Inglês | MEDLINE | ID: mdl-36320391

RESUMO

Reversibility and stability are considered as the key indicators for Zn metal anodes in aqueous Zn-ion batteries, yet they are severely hindered by uncontrolled Zn stripping/plating and side reactions. Herein, we fabricate a bulk phase ZnIn alloy anode containing trace indium by a typical smelting-rolling process. A uniformly dispersed bulk phase of the whole Zn anode is constructed rather than only a protective layer on the surface. The Zn deposition can be regarded as instantaneous nucleation due to the adsorption of the evenly dispersed indium, and formation of the exclusion zone for further nucleation can be prevented at the same time. Owing to the bulk phase structure of ZnIn alloy, the indium not only plays a crucial role in Zn deposition, but also improves the Zn stripping. Consequently, the as-designed ZnIn alloy anode can sustain stable Zn stripping/plating for over 2500 h at 4.4 mA cm-2 with nearly 6 times smaller voltage hysteresis than that of pure Zn. Moreover, it enables a substantially stable ZnIn//NH4V4O10 battery with 96.44% capacity retention after 1000 cycles at 5 A g-1. This method of regulating the Zn nucleation by preparing a Zn-based alloy provides a potential solution to the critical problem of Zn dendrite growth and by-product generation fundamentally.