Your browser doesn't support javascript.
loading
The Study of the Binder Poly(acrylic acid) and Its Role in Concomitant Solid-Electrolyte Interphase Formation on Si Anodes.
Browning, Katie L; Sacci, Robert L; Doucet, Mathieu; Browning, James F; Kim, Joshua R; Veith, Gabriel M.
Afiliação
  • Browning KL; Department of Materials Science and Engineering , University of Tennessee , Knoxville , Tennessee 37996 , United States.
  • Sacci RL; Chemical Sciences Division , Oak Ridge National Laboratory , Oak Ridge , Tennessee 37831 , United States.
  • Doucet M; Chemical Sciences Division , Oak Ridge National Laboratory , Oak Ridge , Tennessee 37831 , United States.
  • Browning JF; Neutron Scattering Division , Oak Ridge National Laboratory , Oak Ridge , Tennessee 37831 , United States.
  • Kim JR; Neutron Scattering Division , Oak Ridge National Laboratory , Oak Ridge , Tennessee 37831 , United States.
  • Veith GM; Neutron Scattering Division , Oak Ridge National Laboratory , Oak Ridge , Tennessee 37831 , United States.
ACS Appl Mater Interfaces ; 12(8): 10018-10030, 2020 Feb 26.
Article em En | MEDLINE | ID: mdl-31984725
ABSTRACT
We use neutron reflectometry to study how the polymeric binder, poly(acrylic acid) (PAA), affects the in situ formation and chemical composition of the solid-electrolyte interphase (SEI) formation on a silicon anode at various states of charge. The reflectivity is correlated with electrochemical quartz crystal microbalance to better understand the viscoelastic effects of the polymer during cycling. The use of model thin films allows for a well-controlled interface between the amorphous Si surface and the PAA layer. If the PAA perfectly coats the Si surface and standard processing conditions are used, the binder will prevent the lithiation of the anode. The PAA suppresses the growth of a new layer formed at early states of discharge (open circuit voltage to 0.8 V vs Li/Li+), protecting the surface of the anode. At 0.15 V, the SEI layer underneath the PAA changes in chemical composition as indicated by an increase in the scattering length density and thickness as the layer incorporates components from the electrolyte, most likely the salt. At lithiated and delithiated states, the SEI layer changes in chemical composition and grows in thickness with delithiation and shrinks during lithiation.