Your browser doesn't support javascript.
loading
Synthesis, Properties, and Biodegradation of Sequential Poly(Ester Amide)s Containing γ-Aminobutyric Acid.
Nakayama, Yuushou; Watanabe, Kazumasa; Tanaka, Ryo; Shiono, Takeshi; Kawasaki, Norioki; Yamano, Naoko; Nakayama, Atsuyoshi.
Afiliação
  • Nakayama Y; Department of Applied Chemistry, Graduate School of Engineering, Hiroshima University, 1-4-1 Kagamiyama, Higashi-Hiroshima, Hiroshima 739-8527, Japan.
  • Watanabe K; Department of Applied Chemistry, Graduate School of Engineering, Hiroshima University, 1-4-1 Kagamiyama, Higashi-Hiroshima, Hiroshima 739-8527, Japan.
  • Tanaka R; Department of Applied Chemistry, Graduate School of Engineering, Hiroshima University, 1-4-1 Kagamiyama, Higashi-Hiroshima, Hiroshima 739-8527, Japan.
  • Shiono T; Department of Applied Chemistry, Graduate School of Engineering, Hiroshima University, 1-4-1 Kagamiyama, Higashi-Hiroshima, Hiroshima 739-8527, Japan.
  • Kawasaki N; Biomedical Research Institute, National Institute of Advanced Industrial Science and Technology (AIST), 1-8-31 Midorigaoka, Ikeda, Osaka 563-8577, Japan.
  • Yamano N; Biomedical Research Institute, National Institute of Advanced Industrial Science and Technology (AIST), 1-8-31 Midorigaoka, Ikeda, Osaka 563-8577, Japan.
  • Nakayama A; Biomedical Research Institute, National Institute of Advanced Industrial Science and Technology (AIST), 1-8-31 Midorigaoka, Ikeda, Osaka 563-8577, Japan.
Int J Mol Sci ; 21(10)2020 May 23.
Article em En | MEDLINE | ID: mdl-32456183
ABSTRACT
Poly(ester amide)s are attracting attention because they potentially have excellent thermal and mechanical properties as well as biodegradability. In this study, we synthesized a series of novel poly(ester amide)s by introducing γ-aminobutyric acid (GABA) regularly into polyesters, and investigated their properties and biodegradabilities. GABA is the monomer unit of biodegradable polyamide 4 (PA4). The new poly(ester amide)s were synthesized from the reaction of ammonium tosylate derivatives of alkylene bis(γ-aminobutylate) and p-nitrophenyl esters of dicarboxylic acids. All the obtained polymers showed relatively high melting temperatures (Tm). Their thermal decomposition temperatures were improved in comparison with that of PA4 and higher enough than their Tm. The poly(ester amide)s exhibited higher biodegradability in seawater than the corresponding homopolyesters. Their biodegradabilities in activated sludge were also studied.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Plásticos Biodegradáveis / Ácido gama-Aminobutírico Idioma: En Revista: Int J Mol Sci Ano de publicação: 2020 Tipo de documento: Article

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Plásticos Biodegradáveis / Ácido gama-Aminobutírico Idioma: En Revista: Int J Mol Sci Ano de publicação: 2020 Tipo de documento: Article