Your browser doesn't support javascript.
loading
Elucidating the Effects of the Composition on Hydrogen Sorption in TiVZrNbHf-Based High-Entropy Alloys.
Ek, Gustav; Nygård, Magnus M; Pavan, Adriano F; Montero, Jorge; Henry, Paul F; Sørby, Magnus H; Witman, Matthew; Stavila, Vitalie; Zlotea, Claudia; Hauback, Bjørn C; Sahlberg, Martin.
Afiliação
  • Ek G; Department of Chemistry - Ångström Laboratory, Uppsala University, Box 523, Uppsala SE-75120, Sweden.
  • Nygård MM; Department for Neutron Materials Characterization, Institute for Energy Technology, P.O. Box 40, Kjeller NO-2027, Norway.
  • Pavan AF; Department of Chemistry - Ångström Laboratory, Uppsala University, Box 523, Uppsala SE-75120, Sweden.
  • Montero J; Institut de Chimie et des Matériaux Paris Est, Université de Paris Est, CNRS, UPEC, Thiais 94320, France.
  • Henry PF; Department of Chemistry - Ångström Laboratory, Uppsala University, Box 523, Uppsala SE-75120, Sweden.
  • Sørby MH; ISIS Pulsed Neutron and Muon Source, Rutherford Appleton Laboratory, Didcot OX11 0QX, United Kingdom.
  • Witman M; Department for Neutron Materials Characterization, Institute for Energy Technology, P.O. Box 40, Kjeller NO-2027, Norway.
  • Stavila V; Sandia National Laboratories, Livermore, California 94551, United States.
  • Zlotea C; Sandia National Laboratories, Livermore, California 94551, United States.
  • Hauback BC; Institut de Chimie et des Matériaux Paris Est, Université de Paris Est, CNRS, UPEC, Thiais 94320, France.
  • Sahlberg M; Department for Neutron Materials Characterization, Institute for Energy Technology, P.O. Box 40, Kjeller NO-2027, Norway.
Inorg Chem ; 60(2): 1124-1132, 2021 Jan 18.
Article em En | MEDLINE | ID: mdl-33370527
ABSTRACT
A number of high-entropy alloys (HEAs) in the TiVZrNbHf system have been synthesized by arc melting and systematically evaluated for their hydrogen sorption characteristics. A total of 21 alloys with varying elemental compositions were investigated, and 17 of them form body-centered-cubic (bcc) solid solutions in the as-cast state. A total of 15 alloys form either face-centered-cubic (fcc) or body-centered-tetragonal (bct) hydrides after exposure to gaseous hydrogen with hydrogen per metal ratios (H/M) as high as 2.0. Linear trends are observed between the volumetric expansion per metal atom [(V/Z)fcc/bct - (V/Z)bcc/hcp]/(V/Z)bcc/hcp with the valence electron concentration and average Pauling electronegativity (χp) of the alloys. However, no correlation was observed between the atomic size mismatch, δ, and any investigated hydrogen sorption property such as the maximum storage capacity or onset temperature for hydrogen release.