Your browser doesn't support javascript.
loading
Marginal and Internal Misfit of Occlusal Veneers Made in Resin-matrix Ceramics.
Ruggiero, M M; Gomes, R S; Bergamo, Etp; Freitas, Mim; Bonfante, E A; Del Bel Cury, A A.
Afiliação
  • Ruggiero MM; Mirelle Maria Ruggiero, DDS, MSc, Department of Prosthodontics and Periodontology, University of Campinas -Piracicaba Dental School, Piracicaba, SP, Brazil.
  • Gomes RS; Rafael Soares Gomes, DDS, MSc, PhD, Department of Prosthodontics and Periodontology, University of Campinas -Piracicaba Dental School, Piracicaba, SP, Brazil.
  • Bergamo E; Edmara Tatiely Pedroso Bergamo, DDS, MSc, PhD, Department of Prosthodontics and Periodontology, University of São Paulo - Bauru School of Dentistry, Bauru, SP, Brazil.
  • Freitas M; Mariana Itaborai Moreira Freitas, DDS, MSc, Department of Prosthodontics and Periodontology, University of Campinas -Piracicaba Dental School, Piracicaba, SP, Brazil.
  • Bonfante EA; Estevam Augusto Bonfante, DDS, MSc, PhD, Department of Prosthodontics and Periodontology, University of São Paulo -Bauru School of Dentistry, Bauru, SP, Brazil.
  • Del Bel Cury AA; *Altair Antoninha Del Bel Cury, DDS, MSc, PhD, Department of Prosthodontics and Periodontology, University of Campinas - Piracicaba Dental School, Piracicaba, SP, Brazil.
Oper Dent ; 47(6): 701-708, 2022 Nov 01.
Article em En | MEDLINE | ID: mdl-36442228
ABSTRACT

OBJECTIVE:

Considering that misfit is a significant predictor of the clinical success of indirect restorations, the objective of this study was to evaluate the marginal and internal misfit of two computer-aided design and manufacturing (CAD/CAM) RMC ceramic materials used as occlusal veneers (OVs) of different thicknesses. METHODS AND MATERIALS A CAD model of a mandibular first molar was obtained and OV preparations 0.5-, 1.0-, and 1.5-mm thick were modeled and milled in two different materials (n=10/group) resin nanoceramic (RNC) and polymer-infiltrated ceramic network (PICN). Using the same CAD model, tooth preparations were milled in fiber-reinforced epoxy resin (n=20/thickness). The marginal and internal misfit of the restorations was assessed by X-ray microtomography. The measurements of the marginal gap (MG) and absolute marginal discrepancy were performed in two locations on each slice, whereas internal gap (IG) measurements were performed at ten locations on each slice. The data obtained were analyzed using two-way analysis of variance and Tukey post-hoc tests (α=0.05).

RESULTS:

No significant effect was attributable to the material type or material-thickness interaction for the MG, absolute marginal discrepancy (AMD), or IG (p>0.05). However, the thickness significantly affected the IG of the restorations (p<0.05). CAD/CAM RNC and PICN systems presented similar MG and AMD for OVs 0.5-, 1.0-, and 1.5-mm thick. However, the IG varied between thicknesses.
Assuntos