Your browser doesn't support javascript.
loading
Structure and properties of chlorogenic acid-loaded polylactide fiber prepared by melt spinning.
Yu, Dongzheng; Duan, Zeping; Wang, Aming; Li, Ling; Guo, Haiyang; Deng, Bingyao; Li, Dawei; Li, Haoxuan; Liu, Qingsheng.
Afiliação
  • Yu D; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Duan Z; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Wang A; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Li L; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Guo H; Jiangsu Doway New Materials Science & Technology Co. Ltd., Suqian 223800, China.
  • Deng B; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Li D; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Li H; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China.
  • Liu Q; Key Laboratory of Eco-Textiles, Ministry of Education, Jiangnan University, Wuxi 214122, China. Electronic address: qsliu@jiangnan.edu.cn.
Int J Biol Macromol ; 265(Pt 1): 130810, 2024 Apr.
Article em En | MEDLINE | ID: mdl-38484822
ABSTRACT
Polylactide/chlorogenic acid (PLA/CGA) blends with different weight ratios were prepared by melt mixing, and corresponding PLA/CGA fibers were produced via a two-step melt spinning process. For PLA/CGA blends, CGA was distributed uniformly in the PLA matrix. The intermolecular interactions between CGA and PLA existed. The viscosity of PLA/CGA blends was much lower than that of neat PLA. With the increase of CGA content, the viscosity of PLA/CGA blends decreased. As the CGA content increased, the crystallinity of both PLA/CGA blends and fibers decreased. In addition, the tensile strength of PLA/CGA fibers was slightly lower than that of neat PLA fiber. For PLA/CGA fibers, the 6-fold drawn PLA/CGA fiber with 3 % CGA owned the highest tensile strength of 420 MPa. The ultraviolet (UV) resistance of PLA/CGA fibers were enhanced significantly by the introduction of CGA. When the CGA content was not <3 %, the UV transmittance of PLA/CGA fibers was <8 %. Moreover, PLA/CGA fibers exhibited good antioxidant properties. PLA/CGA fibers with 10 % CGA owned the highest antioxidant rate of >90 %. In addition, the 6-fold drawn PLA/CGA fiber with 10 % CGA presented excellent release performance with a 7-day cumulative CGA release rate of 19 %.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Ácido Clorogênico / Antioxidantes Idioma: En Revista: Int J Biol Macromol Ano de publicação: 2024 Tipo de documento: Article

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Ácido Clorogênico / Antioxidantes Idioma: En Revista: Int J Biol Macromol Ano de publicação: 2024 Tipo de documento: Article