Effect of Various Plasticizers in Different Concentrations on Physical, Thermal, Mechanical, and Structural Properties of Wheat Starch-Based Films.
Mohammed, Abdulrahman A B A; Hasan, Zaimah; Omran, Abdoulhdi A Borhana; Elfaghi, Abdulhafid M; Khattak, M A; Ilyas, R A; Sapuan, S M.
Afiliação
  • Mohammed AABA; Institute of Sustainable Energy, Universiti Tenaga Nasional, Jalan Ikram-Uniten, Kajang 43000, Selangor, Malaysia.
  • Hasan Z; Institute of Sustainable Energy, Universiti Tenaga Nasional, Jalan Ikram-Uniten, Kajang 43000, Selangor, Malaysia.
  • Omran AAB; Department of Mechanical and Mechatronic Engineering, Faculty of Engineering, Sohar University, Sohar P C-311, Oman.
  • Elfaghi AM; Department of Mechanical Engineering, College of Engineering Science & Technology, Sebha University, Sabha 00218, Libya.
  • Khattak MA; Faculty of Mechanical and Manufacturing Engineering, Universiti Tun Hussein Onn Malaysia, Batu Pahat 86400, Johor, Malaysia.
  • Ilyas RA; ARL Laboratory Services PTY Ltd., 1361/55 Pine Rd., Yennora, Sydney, NSW 216, Australia.
  • Sapuan SM; Faculty of Chemical and Energy Engineering, Universiti Teknologi Malaysia, Johor Bahru 81310, Johor, Malaysia.
Polymers (Basel) ; 15(1)2022 Dec 23.
Article em En | MEDLINE | ID: mdl-36616412
Biocomposite materials are essential for environmental protection, as they have the ability of substituting synthetic plastic with natural materials. This work investigated how different plasticizers (Glycerol (G), Fructose (F), Sorbitol (S), and Urea (U)) affect the morphological, mechanical, thermal, and physical characteristics of films made of wheat starch at various concentrations (0%, 15%, 25%, and 35%). Plasticizers were added to improve the flexibility and homogeneity of the wheat starch-based bioplastic. Control film exhibited high tensile strength (38.7 MPa) with low elongation (1.9%). However, films plasticized with 35% sorbitol showed the highest elongation, which was 60.7% at break. At 35% of all plasticizers, fructose showed the highest tensile strength, with 7.6 MPa. The addition of different plasticizers shows improvement in water resistance; films plasticized with glycerol had the lowest water absorption at 35% fructose (187.4%) and also showed coherent surfaces. Glycerol, sorbitol, and urea films showed a higher mass loss compared to fructose films. Fructose showed the highest performance after the analysis of the results, with low water absorption, water content, and mass loss and with high mechanical performance at 35% of fructose. SEM images show that the addition of fructose and glycerol improves the surface homogenate, while sorbitol and urea have a less compact structure with large pores.