Boosted Oxygen Kinetics of Hierarchically Mesoporous Mo2C/C for High-current-density Zn-air Battery.
Zhang, Jun-Ye; Xia, Chenfeng; Su, Yaqiong; Zu, Lianhai; Zhao, Zaiwang; Li, Peng; Lv, Zirui; Wang, Jiazheng; Mei, Bingbao; Lan, Kun; Zhao, Tiancong; Zhang, Pengfei; Chen, Weinan; Zaman, Shahid; Liu, Yi; Peng, Liang; Xia, Bao Yu; Elzatahry, Ahmed; Li, Wei; Zhao, Dongyuan.
Afiliación
  • Zhang JY; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Xia C; School of Chemistry and Chemical Engineering, Huazhong University of Science and Technology, 1037 Luoyu Road, Wuhan, 430074, P. R. China.
  • Su Y; School of Chemistry, Xi'an Jiaotong University, Xi'an, 710049, P. R. China.
  • Zu L; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Zhao Z; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Li P; School of Chemistry, Xi'an Jiaotong University, Xi'an, 710049, P. R. China.
  • Lv Z; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Wang J; College of Chemistry and Chemical Engineering, Xiamen University, Xiamen, 361005, P. R. China.
  • Mei B; Shanghai Institute of Applied Physics, Shanghai Synchrotron Radiation Facility, Chinese Academy of Sciences, Shanghai, 201204, P. R. China.
  • Lan K; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Zhao T; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Zhang P; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Chen W; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Zaman S; School of Chemistry and Chemical Engineering, Huazhong University of Science and Technology, 1037 Luoyu Road, Wuhan, 430074, P. R. China.
  • Liu Y; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Peng L; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Xia BY; School of Chemistry and Chemical Engineering, Huazhong University of Science and Technology, 1037 Luoyu Road, Wuhan, 430074, P. R. China.
  • Elzatahry A; Department of Physics and Materials Science, College of Arts and Sciences, Qatar University, PO Box 2713, Doha, 2713, Qatar.
  • Li W; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
  • Zhao D; Laboratory of Advanced Materials, Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, School of Chemistry and Materials, Fudan University, Shanghai, 200433, P. R. China.
Small ; 20(15): e2307378, 2024 Apr.
Article en En | MEDLINE | ID: mdl-38009801

Texto completo: 1 Colección: 01-internacional Banco de datos: MEDLINE Idioma: En Revista: Small Asunto de la revista: ENGENHARIA BIOMEDICA Año: 2024 Tipo del documento: Article

Texto completo: 1 Colección: 01-internacional Banco de datos: MEDLINE Idioma: En Revista: Small Asunto de la revista: ENGENHARIA BIOMEDICA Año: 2024 Tipo del documento: Article