Flexibility of Poly(alkyl methacrylate)s Characterized by Their Persistence Length Determined through Pyrene Excimer Formation.
Lulic, Kristijan; Muller, Grégoire; Gutierrez, Renzo; Little, Hunter; Duhamel, Jean.
Afiliación
  • Lulic K; Institute for Polymer Research, Waterloo Institute for Nanotechnology, Department of Chemistry, University of Waterloo, 200 University Avenue West, Waterloo, ON N2L 3G1, Canada.
  • Muller G; Institute for Polymer Research, Waterloo Institute for Nanotechnology, Department of Chemistry, University of Waterloo, 200 University Avenue West, Waterloo, ON N2L 3G1, Canada.
  • Gutierrez R; Institute for Polymer Research, Waterloo Institute for Nanotechnology, Department of Chemistry, University of Waterloo, 200 University Avenue West, Waterloo, ON N2L 3G1, Canada.
  • Little H; Institute for Polymer Research, Waterloo Institute for Nanotechnology, Department of Chemistry, University of Waterloo, 200 University Avenue West, Waterloo, ON N2L 3G1, Canada.
  • Duhamel J; Institute for Polymer Research, Waterloo Institute for Nanotechnology, Department of Chemistry, University of Waterloo, 200 University Avenue West, Waterloo, ON N2L 3G1, Canada.
Polymers (Basel) ; 16(15)2024 Jul 26.
Article en En | MEDLINE | ID: mdl-39125153
ABSTRACT
A series of poly(alkyl methacrylate)s and poly(oligo(ethylene glycol) methyl ether methacrylate)s labeled with 1-pyrenebutanol were referred to as the PyC4-PCnMA samples with n = 1, 4, 6, 8, 12, and 18 and the PyC4-PEGnMA samples with n = 0-5, 9, 16, and 19, respectively. Pyrene excimer formation (PEF) upon the encounter between an excited and a ground-state pyrenyl labels was employed to determine their persistence length (lp) in o-xylene. The fluorescence decays of the PyC4-PCnMA and PyC4-PEGnMA samples were acquired and analyzed with the fluorescence blob model to yield the number (Nblob) of structural units in the volume probed by an excited pyrenyl label. Nblob was found to decrease with an increasing number (NS) of non-hydrogen atoms in the side chain, reaching a plateau for the PyC4-PEGnMA samples with a longer side chain (n = 16 and 19). The Nblob values were used to determine lp. The lp values for the PyC4-PCnMA and PyC4-PEGnMA samples increased linearly with increasing NS2 as predicted theoretically, which agreed with the lp values obtained by viscometry for a series of PCnMA samples. The good agreement between the lp values retrieved by PEF and viscometry served to validate the PEF-based methodology for determining lp for linear polymers.