Do ozonated water and boric acid affect the bond strength to dentin in different adhesive systems?
Akturk, E; Bektas, O O; Ozkanoglu, S; G Akin, E G.
Afiliação
  • Akturk E; Department of Restorative Dentistry, Faculty of Dentistry, Cumhuriyet University, Sivas, Turkey.
  • Bektas OO; Department of Restorative Dentistry, Faculty of Dentistry, Cumhuriyet University, Sivas, Turkey.
  • Ozkanoglu S; Department of Restorative Dentistry, Faculty of Dentistry, Cumhuriyet University, Sivas, Turkey.
  • G Akin EG; Department of Restorative Dentistry, Faculty of Dentistry, Sakarya Univercity, Sakarya, Turkey.
Niger J Clin Pract ; 22(12): 1758-1764, 2019 Dec.
Article em En | MEDLINE | ID: mdl-31793485
ABSTRACT

AIM:

The aim of this in vitro study was to compare the effects of the application of three different cavity disinfecting agents to dentin on the micro-shear bond strength (µ-SBS) of one self-etch and two universal adhesive systems. MATERIALS AND

METHODS:

In total, 120 caries-free human permanent molar teeth were used in this study. Mid-coronal dentin surfaces were revealed by cutting occlusal enamel and a standard smear layer was obtained by using 600-800-1200 grid silicon carbide abrasive papers. Specimens were randomly assigned to four groups according to the disinfectant used Group 1 Control (no disinfectant); Group 2 2% chlorhexidine based (Consepsis); Group 3 10 ppm ozonated water (TeknO3zone); Group 4 5% boric acid (Handmade). Each group was divided into three subgroups according to the type of adhesive (Clearfil SE Bond, OptiBond XTR, and Tokuyama Universal). Specimens were bonded using either Clearfil SE Bond, OptiBond XTR or Tokuyama Universal, which were employed according to the manufacturer's instructions. Resin composite microcylinders were bonded using Tygon® tubes for µ-SBS testing. After specimens were stored for 24 h, at 37°C in distilled water, µ-SBS test was measured with a universal test machine (LF Plus, Lloyd, Instrument). µ-SBS results were analyzed by one-way analysis of variance (ANOVA) and Tukey's tests.

RESULTS:

When the mean microshear bond strength values of the control group were compared, the difference between the subgroups was not significant (P < 0.05). When the mean microshear bond strength values of the chx, ozonated water, and boric acid were compared, the difference between Clearfil SE Bond and Tokuyama Universal was significant (P < 0.05) and the difference between the other groups was not significant (P > 0.05).

CONCLUSION:

Ozonated water and boric acid may be as an alternative to other materials used as cavity disinfectants.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Ácidos Bóricos / Água / Colagem Dentária / Adesivos Dentinários / Desinfetantes de Equipamento Odontológico / Cimentos Dentários / Dentina Tipo de estudo: Clinical_trials Limite: Humans Idioma: En Revista: Niger J Clin Pract Assunto da revista: MEDICINA Ano de publicação: 2019 Tipo de documento: Article País de afiliação: Turquia

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Ácidos Bóricos / Água / Colagem Dentária / Adesivos Dentinários / Desinfetantes de Equipamento Odontológico / Cimentos Dentários / Dentina Tipo de estudo: Clinical_trials Limite: Humans Idioma: En Revista: Niger J Clin Pract Assunto da revista: MEDICINA Ano de publicação: 2019 Tipo de documento: Article País de afiliação: Turquia