Impact of Humidity and Temperature on the Stability of the Optical Properties and Structure of MAPbI3, MA0.7FA0.3PbI3 and (FAPbI3)0.95(MAPbBr3)0.05 Perovskite Thin Films.
Tumusange, Marie Solange; Subedi, Biwas; Chen, Cong; Junda, Maxwell M; Song, Zhaoning; Yan, Yanfa; Podraza, Nikolas J.
Afiliação
  • Tumusange MS; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
  • Subedi B; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
  • Chen C; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
  • Junda MM; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
  • Song Z; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
  • Yan Y; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
  • Podraza NJ; Department of Physics & Astronomy and The Wright Center for Photovoltaics Innovation & Commercialization, University of Toledo, Toledo, OH 43606, USA.
Materials (Basel) ; 14(14)2021 Jul 20.
Article em En | MEDLINE | ID: mdl-34300973
In situ real-time spectroscopic ellipsometry (RTSE) measurements have been conducted on MAPbI3, MA0.7FA0.3PbI3, and (FAPbI3)0.95(MAPbBr3)0.05 perovskite thin films when exposed to different levels of relative humidity at given temperatures over time. Analysis of RTSE measurements track changes in the complex dielectric function spectra and structure, which indicate variations in stability influenced by the underlying material, preparation method, and perovskite composition. MAPbI3 and MA0.7FA0.3PbI3 films deposited on commercial fluorine-doped tin oxide coated glass are more stable than corresponding films deposited on soda lime glass directly. (FAPbI3)0.95(MAPbBr3)0.05 films on soda lime glass showed improved stability over the other compositions regardless of the substrate, and this is attributed to the preparation method as well as the final composition.