1.
Chem Commun (Camb)
; (12): 1416-7, 2004 Jun 21.
Artigo
em Inglês
| MEDLINE
| ID: mdl-15179492
RESUMO
Highly purified cobalt colloids have been employed as a catalyst to grow aligned carbon nanofibres at temperatures as low as 300 degree C by dc plasma enhanced chemical vapour deposition over large areas.
2.
Chem Commun (Camb)
; 50(77): 11343-6, 2014 Oct 07.
Artigo
em Inglês
| MEDLINE
| ID: mdl-25164378
RESUMO
The synthesis of nitrogenated carbon nanotubes (N-CNTs) with up to 6.1 wt% N, via the use of pyridine as the nitrogen containing carbon precursor, can provide a facile route to significantly enhance the low intrinsic specific capacitance of carbon nanotubes. The nitrogen functionalities determine this, at least, five-fold increase of the specific capacitance.