Your browser doesn't support javascript.
loading
Highly Durable PtNi Alloy on Sb-Doped SnO2 for Oxygen Reduction Reaction with Strong Metal-Support Interaction.
Fang, Liwei; Wang, Shengsen; Lu, Yiqing; Deng, Chengwei; Sun, Liping; Cheng, Yuanhui.
Afiliação
  • Fang L; State Key Laboratory of Organic-Inorganic Composites, College of Chemical Engineering, Beijing University of Chemical Technology, Beijing, 100029, P. R. China.
  • Wang S; State Key Laboratory of Organic-Inorganic Composites, College of Chemical Engineering, Beijing University of Chemical Technology, Beijing, 100029, P. R. China.
  • Lu Y; State Key Laboratory of Organic-Inorganic Composites, College of Chemical Engineering, Beijing University of Chemical Technology, Beijing, 100029, P. R. China.
  • Deng C; State Key Laboratory of Space Power-Sources Technology, Shanghai Institute of Space Power Sources, Shanghai, 200245, P. R. China.
  • Sun L; China Energy Technology and Economics Research Institute, China Energy Investment Corporation Ltd., Beijing, 102211, P. R. China.
  • Cheng Y; State Key Laboratory of Organic-Inorganic Composites, College of Chemical Engineering, Beijing University of Chemical Technology, Beijing, 100029, P. R. China.
Chem Asian J ; 18(20): e202300601, 2023 Oct 17.
Article em En | MEDLINE | ID: mdl-37646223
ABSTRACT
Carbon-supported Pt is currently used as catalyst for oxygen reduction reaction (ORR) in fuel cells but is handicapped by carbon corrosion at high potential. Herein, a stable PtNi/SnO2 interface structure has been designed and achieved by a two-step solvothermal method. The robust and conductive Sb-doped SnO2 supports provide sufficient surfaces to confine PtNi alloy. Moreover, PtNi/Sb0.11 SnO2 presents a more strongly coupled Pt-SnO2 interface with lattice overlap of Pt (111) and SnO2 (110), together with enhanced electron transfer from SnO2 to Pt. Therefore, PtNi/Sb0.11 SnO2 exhibits a high catalytic activity for ORR with a half-wave potential of 0.860 V versus reversible hydrogen electrode (RHE) and a mass activity of 166.2 mA mgPt -1 @0.9 V in 0.1 M HClO4 electrolyte. Importantly, accelerated degradation testing (ADT) further identify the inhibition of support corrosion and agglomeration of Pt-based active nanoparticles in PtNi/Sb0.11 SnO2 . This work highlights the significant importance of modulating metal-support interactions for improving the catalytic activity and durability of electrocatalysts.