Your browser doesn't support javascript.
loading
Self-Assembly of Silicon Nanotubes Driven by a Biphasic Transition from the Natural Mineral Montmorillonite in Molten Salt Electrolysis.
Wang, Fan; Liu, Wei; Li, Peng; Guan, Ziheng; Li, Wei; Wang, Dihua.
Afiliação
  • Wang F; School of Resource and Environmental Sciences, Hubei International Scientific and Technological Cooperation Base of Sustainable Resource and Energy, Wuhan University, Wuhan, 430072, P. R. China.
  • Liu W; College of Chemistry and Materials Engineering, Zhejiang A&F University, Hangzhou, 311300, P. R. China.
  • Li P; School of Resource and Environmental Sciences, Hubei International Scientific and Technological Cooperation Base of Sustainable Resource and Energy, Wuhan University, Wuhan, 430072, P. R. China.
  • Guan Z; School of Resource and Environmental Sciences, Hubei International Scientific and Technological Cooperation Base of Sustainable Resource and Energy, Wuhan University, Wuhan, 430072, P. R. China.
  • Li W; School of Resource and Environmental Sciences, Hubei International Scientific and Technological Cooperation Base of Sustainable Resource and Energy, Wuhan University, Wuhan, 430072, P. R. China.
  • Wang D; College of Chemistry and Materials Engineering, Zhejiang A&F University, Hangzhou, 311300, P. R. China.
Small ; : e2311334, 2024 Feb 25.
Article em En | MEDLINE | ID: mdl-38402440
ABSTRACT
Silicon nanotubes (SNTs) have been considered as promising anode materials for lithium-ion batteries (LIBs). However, the reported strategies for preparing SNTs generally have special requirements for either expensive templates or complex catalysts. It is necessary to explore a cost-effective and efficient approach for the preparation of high-performance SNTs. In this work, a biphasic transformation strategy involving "solid-state reduction" and "dissolution-deposition" in molten salts is developed to prepare SNTs using montmorillonite as a precursor. The rod-like intermediate of silicon-aluminum-calcium is initially reduced in solid state, which then triggers the continuous dissolution and deposition of calcium silicate in the inner space of the intermediate to form a hollow structure during the subsequent reduction process. The transition from solid to liquid is crucial for improving the kinetics of deoxygenation and induces the self-assembly of SNTs during electrolysis. When the obtained SNTs is used as anode materials for LIBs, they exhibit a high capacity of 2791 mAh g-1 at 0.2 A g-1 , excellent rate capability of 1427 mA h g-1 at 2 A g-1 , and stable cycling performance with a capacity of 2045 mAh g-1 after 200 cycles at 0.5 A g-1 . This work provides a self-assembling, controllable, and cost-effective approach for fabricating SNTs.
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Idioma: En Revista: Small Assunto da revista: ENGENHARIA BIOMEDICA Ano de publicação: 2024 Tipo de documento: Article