Minimizing Undesired Side Reactions Induced by Nanoscale Conductive Carbon Enables Stable Cycling of Semi-Solid Li-Ion Full Batteries.
Chen, Hongli; Wang, Yong; Meng, Dechao; Zhu, Yingying; He, Yu-Shi; Ma, Zi-Feng; Li, Linsen.
Afiliação
  • Chen H; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
  • Wang Y; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
  • Meng D; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
  • Zhu Y; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
  • He YS; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
  • Ma ZF; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
  • Li L; Department of Chemical Engineering, Shanghai Electrochemical Energy Devices Research Center (SEED), School of Chemistry and Chemical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, China.
Small ; : e2403674, 2024 Jul 28.
Article em En | MEDLINE | ID: mdl-39072991
ABSTRACT
Semi-solid lithium-ion batteries (SSLIBs) based on "slurry-like" electrodes hold great promise to enable low-cost and sustainable energy storage. However, the development of the SSLIBs has long been hindered by the lack of high-performance anodes. Here the origin of low initial Coulombic efficiency (iCE, typically <60%) is elucidated in the graphite-based semi-solid anodes (in the non-flowing mode) and develop rational strategies to minimize the irreversible capacity loss. It is discovered that Ketjen black (KB), a nanoscale conductive additive widely used in SSLIB research, induces severe electrolyte decomposition during battery charge due to its large surface area and abundant surface defects. High iCEs up to 92% are achieved for the semi-solid graphite anodes by replacing KB with other low surface-area, low-defect conductive additives. A semi-solid full battery (LiFePO4 vs graphite, in the non-flowing mode) is further demonstrated with stable cycle performance over 100 cycles at a large areal capacity of 6 mAh cm-2 and a pouch-type semi-solid full cell that remains functional even when it is mechanically abused. This work demystifies the SSLIBs and provides useful physical insights to further improve their performance and durability.