Your browser doesn't support javascript.
loading
Effect of polishing and bleaching on color, whiteness, and translucency of CAD/CAM monolithic materials.
Peña, Ranulfo Castillo; Ramos, Alejandro Cardenas; Dos Santos Nunes Reis, José Maurício; Dovigo, Lívia Nordi; Salomon, Jean-Pierre Guy Olivier; Del Mar Pérez, María; Fonseca, Renata Garcia.
Afiliação
  • Peña RC; Department of Dental Materials and Prosthodontics, Araraquara Dental School, UNESP-Univ. Estadual Paulista, Araraquara, São Paulo, Brazil.
  • Ramos AC; Department of Dental Materials and Prosthodontics, Araraquara Dental School, UNESP-Univ. Estadual Paulista, Araraquara, São Paulo, Brazil.
  • Dos Santos Nunes Reis JM; Department of Dental Materials and Prosthodontics, Araraquara Dental School, UNESP-Univ. Estadual Paulista, Araraquara, São Paulo, Brazil.
  • Dovigo LN; Department of Social Dentistry, São Paulo State University (UNESP), School of Dentistry, Araraquara, Brazil.
  • Salomon JGO; Department of Medical Devices and Dental Biomaterials, Nancy's Dental Faculty, University of Lorraine, France.
  • Del Mar Pérez M; Department of Optics, School of Science, University of Granada, IBS Campus Fuente Nueva, Granada, Spain.
  • Fonseca RG; Department of Dental Materials and Prosthodontics, Araraquara Dental School, UNESP-Univ. Estadual Paulista, Araraquara, São Paulo, Brazil.
J Esthet Restor Dent ; 2024 Jul 30.
Article em En | MEDLINE | ID: mdl-39076158
ABSTRACT

OBJECTIVE:

To evaluate the effect of polishing and bleaching on the recovery of lightness, color, whiteness, and relative translucency parameter (RTP) in CAD/CAM materials and changes in these properties when another staining in coffee was conducted after the treatments. MATERIALS AND

METHODS:

Disks of Lava Ultimate (LU), Vita Enamic (VE), IPS Empress CAD (EMP), IPS e.max CAD (EMAX), and Vita Suprinity (VS) were (1) not treated (control), (2) polished with Proxyt or (3) Ceramisté, (4) bleached with Opalescence PF or (5) Whiteness HP Blue, and (6) air polished with Clinpro Prophy Powder. CIE L*a*b* color coordinates were registered at baseline (R0), after staining with coffee for 30 min daily for 36.5 days and treatment (R1), and after another staining (R2). Differences (R1-R0 and R2-R0) in lightness (ΔL00), color (ΔE00), RTP (ΔRTP00), and whiteness (ΔWID) were evaluated by mixed repeated measures ANOVA and 95% confidence intervals (α = 0.05) and interpreted in function of their respective 5050% PT and AT thresholds. Topography was evaluated by scanning electron microscopy (SEM).

RESULTS:

In LU, Opalescence PF and Proxyt decreased Δ L 00 R 1 - R 0 $$ {\Delta L}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ , Δ E 00 R 1 - R 0 $$ {\Delta E}_{00\left({R}_1\hbox{--} {\mathrm{R}}_0\right)} $$ , and ΔWI D R 1 - R 0 $$ {\Delta \mathrm{WI}}_{\mathrm{D}\left({R}_1\hbox{--} {R}_0\right)} $$ and showed lower Δ L 00 R 2 - R 0 $$ {\Delta L}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ , Δ E 00 R 2 - R 0 $$ {\Delta E}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ , and ΔWI D R 2 - R 0 $$ {\Delta \mathrm{WI}}_{\mathrm{D}\left({R}_2\hbox{--} {R}_0\right)} $$ . In VE, all treatments decreased Δ L 00 R 1 - R 0 $$ {\Delta L}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ , Δ E 00 R 1 - R 0 $$ {\Delta E}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ , and ΔWI D R 1 - R 0 $$ {\Delta \mathrm{WI}}_{\mathrm{D}\left({R}_1\hbox{--} {R}_0\right)} $$ , whereas Δ L 00 R 2 - R 0 $$ {\Delta L}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ , Δ E 00 R 2 - R 0 $$ {\Delta E}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ , and ΔWI D R 2 - R 0 $$ {\Delta \mathrm{WI}}_{\mathrm{D}\left({R}_2\hbox{--} {R}_0\right)} $$ were lower in Opalescence PF than in the control group. In both moments, ΔE00 and ΔWID in EMP (also ΔL00) and EMAX were higher in Opalescence PF than in the control group, from which the other treatments did not differ in R1-R0. In EMP, Δ E 00 R 2 - R 0 $$ {\Delta E}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ in Whiteness HP Blue (also Δ L 00 R 2 - R 0 $$ {\Delta L}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ ) and Proxyt were also higher in comparison to the control group and in VS, Ceramisté decreased Δ L 00 R 1 - R 0 $$ {\Delta L}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ , Δ E 00 R 1 - R 0 $$ {\Delta E}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ , and Δ R T P 00 R 1 - R 0 $$ \varDelta RT{P}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ , whereas Opalescence PF increased ΔRTP 00 R 1 - R 0 $$ {\Delta \mathrm{RTP}}_{00\left({R}_1\hbox{--} {R}_0\right)} $$ . Δ E 00 R 2 - R 0 $$ {\Delta E}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ of Ceramisté and ΔWI D R 2 - R 0 $$ {\Delta \mathrm{WI}}_{\mathrm{D}\left({R}_2\hbox{--} {R}_0\right)} $$ and Δ R T P 00 R 2 - R 0 $$ \varDelta RT{P}_{00\left({R}_2\hbox{--} {R}_0\right)} $$ of Proxyt were lower than those of the control group.

CONCLUSIONS:

The most suitable treatment to recover the lightness, color, whiteness, and RTP without changing these properties after another coffee exposure is material-dependent. CLINICAL

SIGNIFICANCE:

Although the effectiveness of the treatment was material-dependent, Proxyt was the only treatment that promoted clinically acceptable changes for both LU and VE, while for purely ceramic materials, this condition was observed with Ceramisté and Clinpro Prophy Powder.