A comparison of the marginal fit of In-Ceram, IPS Empress, and Procera crowns.
Int J Prosthodont
; 10(5): 478-84, 1997.
Article
em En
| MEDLINE
| ID: mdl-9495168
ABSTRACT
The in vitro marginal fit of three all-ceramic crown systems (In-Ceram, Procera, and IPS Empress) was compared. All crown systems were significantly different from each other at P = 0.05. In-Ceram exhibited the greatest marginal discrepancy (161 microns), followed by Procera (83 microns), and IPS Empress (63 microns). There were no significant differences among the various stages of the crown fabrication core fabrication, porcelain veneering, and glazing. The facial and lingual margins exhibited significantly larger marginal discrepancies than the mesial and distal margins.
Buscar no Google
Coleções:
01-internacional
Base de dados:
MEDLINE
Assunto principal:
Titânio
/
Ligas Metalo-Cerâmicas
/
Adaptação Marginal Dentária
/
Coroas
/
Porcelana Dentária
/
Óxido de Alumínio
/
Silicatos de Alumínio
Limite:
Humans
Idioma:
En
Revista:
Int J Prosthodont
Assunto da revista:
ODONTOLOGIA
Ano de publicação:
1997
Tipo de documento:
Article
País de afiliação:
Estados Unidos