Your browser doesn't support javascript.
loading
Examining Electrolyte Compatibility on Polymorphic MnO2 Cathodes for Room-Temperature Rechargeable Magnesium Batteries.
Ye, Xiatong; Li, Hongyi; Hatakeyama, Takuya; Kobayashi, Hiroaki; Mandai, Toshihiko; Okamoto, Norihiko L; Ichitsubo, Tetsu.
Afiliación
  • Ye X; Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan.
  • Li H; Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan.
  • Hatakeyama T; Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan.
  • Kobayashi H; Institute of Multidisciplinary Research for Advanced Materials, Tohoku University, Sendai 980-8577, Japan.
  • Mandai T; Center for Green Research on Energy and Environmental Materials, National Institute for Materials Science (NIMS), Tsukuba, Ibaraki 305-0044, Japan.
  • Okamoto NL; Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan.
  • Ichitsubo T; Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan.
ACS Appl Mater Interfaces ; 14(51): 56685-56696, 2022 Dec 28.
Article en En | MEDLINE | ID: mdl-36521016
ABSTRACT
Rechargeable magnesium batteries are promising candidates for post-lithium-ion batteries, owing to the large source abundance and high theoretical energy density. However, there remain few reports on constructing practical cells with oxide cathodes and Mg anodes at room temperature. In this work, we compare the reaction behavior of various MnO2 polymorph cathodes in two representative electrolytes Mg[TFSA]2/G3 and Mg[Al(hfip)4]2/G3. In Mg[TFSA]2/G3, discharge capacities of the MnO2 cathodes are well consistent with the changes in Mg composition, where nanorod-like α-MnO2 and λ-MnO2 show the capacities of about 100 mA h g-1 at room temperature. However, this electrolyte has the disadvantage that the Mg anodes are easily passivated. In contrast, Mg[Al(hfip)4]2/G3 allows highly reversible deposition/dissolution of Mg anodes, whereas the discharge process of the MnO2 cathodes involves a large part of side reactions, in which the MnO2 active material takes part in some reductive reaction together with electrolyte species instead of the expected Mg2+ intercalation. Such an unstable electrode/electrolyte interface would lead to continuous degradation on/near the cathode surface. Thus, the interfacial stability between the oxide cathodes and the electrolytes must be improved for practical applications.