RESUMO
X-ray near-field speckle-based phase-sensing approaches provide efficient means of characterizing optical elements. Presented here is a theoretical review of several of these speckle methods within the framework of optical characterization, and a generalization of the concept is provided. As is also demonstrated experimentally in a parallel paper [Berujon, Cojocaru, Piault, Celestre, Roth, Barrett & Ziegler (2020), J. Synchrotron Rad. 27, (this issue)], the methods theoretically developed here can be applied to different beams and optics and within a variety of situations where at-wavelength metrology is desired. By understanding the differences between the various processing methods, it is possible to find and implement the most suitable approach for each metrology scenario.
RESUMO
A parallel paper [Berujon, Cojocaru, Piault, Celestre, Roth, Barrett & Ziegler (2020), J. Synchrotron Rad. 27, 284-292] reviewed theoretically some of the available processing schemes for X-ray wavefront sensing based on random modulation. Shown here are experimental applications of the technique for characterizing both refractive and reflective optical components. These fast and accurate X-ray at-wavelength metrology methods can assist the manufacture of X-ray optics that transport X-ray beams with a minimum amount of wavefront distortion. It is also recalled how such methods can facilitate online optimization of active optics.
RESUMO
In the present study, in-situ observation of Hot Isostatic Pressure (HIP) procedure of laser powder bed fusion manufactured Ti-6Al-4V parts was performed to quantitatively estimate the densification rate of the material and the influence of the defect initial size and shape on such rate. The observations were performed in-situ using the Ultrafast Tomography Paris-Edinburgh Cell and the combination of fast phase-contrast synchrotron X-ray tomography and energy dispersive diffraction. With this strategy, we could quantify how the effectiveness of HIP depends on the characteristics of a defect. Smaller defects showed a higher densification rate, while the defect shape did not have significant effect on such rate.