Bio-Based, Recyclable and Self-Healing Polyurethane Composites with High Energy Dissipation and Shape Memory.
Shou, Tao; Zhai, Mengyao; Wu, Yaowen; Wu, Sizhu; Hu, Shikai; Zhao, Xiuying; Zhang, Liqun.
Afiliação
  • Shou T; State Key Laboratory of Organic-Inorganic Composites, Beijing University of Chemical Technology, Beijing, 100029, China.
  • Zhai M; Beijing Engineering Research Center of Advanced Elastomers, Beijing University of Chemical Technology, Beijing, 100029, China.
  • Wu Y; State Key Laboratory of Organic-Inorganic Composites, Beijing University of Chemical Technology, Beijing, 100029, China.
  • Wu S; Beijing Engineering Research Center of Advanced Elastomers, Beijing University of Chemical Technology, Beijing, 100029, China.
  • Hu S; State Key Laboratory of Organic-Inorganic Composites, Beijing University of Chemical Technology, Beijing, 100029, China.
  • Zhao X; Beijing Engineering Research Center of Advanced Elastomers, Beijing University of Chemical Technology, Beijing, 100029, China.
  • Zhang L; State Key Laboratory of Organic-Inorganic Composites, Beijing University of Chemical Technology, Beijing, 100029, China.
Macromol Rapid Commun ; 43(21): e2200486, 2022 Nov.
Article em En | MEDLINE | ID: mdl-35947533
ABSTRACT
Rubber composites make an important contribution to eliminating vibration and noise owing to their unique viscoelasticity. However, it is important to find alternative bio-based products with high damping properties owing to the shortage of petrochemical resources and poor performance. The ability to self-heal is an additional characteristic that is highly desirable because it can further increase the service life and safety of such products. In this study, a bio-based polylactic acid thermoplastic polyurethane (PLA-TPU) and its composites (PLA-TPU/AO-80) are synthesized. The reversible sacrificial hydrogen bonds in the composites increase the peak value of the loss factor (tan δmax ) from 0.87 to 2.12 with a high energy dissipation efficiency of 99% at 50% strain. After being heated for 15 min, the healed sample recovers 81.98% of its comprehensive mechanical properties due to the reorganization of the hydrogen bonds. Its tensile strength remains at 93.4% after recycling five times. Moreover, its shape memory properties show a response temperature close to the human body temperature making it an ideal candidate for medical applications.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Poliésteres / Poliuretanos Limite: Humans Idioma: En Revista: Macromol Rapid Commun Ano de publicação: 2022 Tipo de documento: Article País de afiliação: China

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Poliésteres / Poliuretanos Limite: Humans Idioma: En Revista: Macromol Rapid Commun Ano de publicação: 2022 Tipo de documento: Article País de afiliação: China