Nanostructuring Biobased Epoxy Resin with PEO-PPO-PEO Block Copolymer.
Barandiaran, Irati; Gomez-Hermoso-de-Mendoza, Joseba; Gutierrez, Junkal; Tercjak, Agnieszka; Kortaberria, Galder.
Afiliação
  • Barandiaran I; Group 'Materials + Technologies' (GMT), Chemical and Environmental Engineering Department, Faculty of Engineering of Gipuzkoa, University of the Basque Country (UPV/EHU), Plaza Europa 1, 20018 Donostia-San Sebastian, Spain.
  • Gomez-Hermoso-de-Mendoza J; Chemical and Environmental Engineering Department, Faculty of Pharmacy, University of the Basque Country (UPV/EHU), Paseo de la Universidad, 7, 01006 Vitoria-Gasteiz, Spain.
  • Gutierrez J; Group 'Materials + Technologies' (GMT), Chemical and Environmental Engineering Department, Faculty of Engineering of Gipuzkoa, University of the Basque Country (UPV/EHU), Plaza Europa 1, 20018 Donostia-San Sebastian, Spain.
  • Tercjak A; Group 'Materials + Technologies' (GMT), Chemical and Environmental Engineering Department, Faculty of Engineering of Gipuzkoa, University of the Basque Country (UPV/EHU), Plaza Europa 1, 20018 Donostia-San Sebastian, Spain.
  • Kortaberria G; Group 'Materials + Technologies' (GMT), Chemical and Environmental Engineering Department, Faculty of Engineering of Gipuzkoa, University of the Basque Country (UPV/EHU), Plaza Europa 1, 20018 Donostia-San Sebastian, Spain.
Polymers (Basel) ; 15(5)2023 Feb 28.
Article em En | MEDLINE | ID: mdl-36904457
A biobased diglycidyl ether of vanillin (DGEVA) epoxy resin was nanostructured by poly(ethylene oxide-b-propylene oxide-b-ethylene oxide) (PEO-PPO-PEO) triblock copolymer. Due to the miscibility/immiscibility properties of the triblock copolymer in DGEVA resin, different morphologies were obtained depending on the triblock copolymer amount. A hexagonally packed cylinder morphology was kept until reaching 30 wt% of PEO-PPO-PEO content, while a more complex three-phase morphology was obtained for 50 wt%, in which large worm-like PPO domains appear surrounded by two different phases, one of them rich in PEO and another phase rich in cured DGEVA. UV-vis measurements show that the transmittance is reduced with the increase in triblock copolymer content, especially at 50 wt%, probably due to the presence of PEO crystals detected by calorimetry.