Self-Assembly and In Situ Quaternization of Triblock Bottlebrush Block Copolymers via Organized Spontaneous Emulsification for Effective Loading of DNA.
Wang, Zhaoxu; Liu, Qiujun; Liu, Qian; Qi, Hao; Li, Yuesheng; Song, Dong-Po.
Afiliação
  • Wang Z; Tianjin Key Laboratory of Composite and Functional Materials, School of Materials Science and Engineering, Tianjin University, Tianjin, 300350, P. R. China.
  • Liu Q; Tianjin Key Laboratory of Composite and Functional Materials, School of Materials Science and Engineering, Tianjin University, Tianjin, 300350, P. R. China.
  • Liu Q; School of Chemical Engineering and Technology, Tianjin University, Tianjin, 300072, P. R. China.
  • Qi H; School of Chemical Engineering and Technology, Tianjin University, Tianjin, 300072, P. R. China.
  • Li Y; Tianjin Key Laboratory of Composite and Functional Materials, School of Materials Science and Engineering, Tianjin University, Tianjin, 300350, P. R. China.
  • Song DP; Tianjin Key Laboratory of Composite and Functional Materials, School of Materials Science and Engineering, Tianjin University, Tianjin, 300350, P. R. China.
Macromol Rapid Commun ; 44(23): e2300192, 2023 Dec.
Article em En | MEDLINE | ID: mdl-37194368
ABSTRACT
Microspheres bearing large pores are useful in the capture and separation of biomolecules. However, pore size is typically poorly controlled, leading to disordered porous structures with limited performances. Herein, ordered porous spheres with a layer of cations on the internal surface of the nanopores are facilely fabricated in a single step for effective loading of DNA bearing negative charges. Triblock bottlebrush copolymers (BBCPs), (polynorbornene-g-polystyrene)-b-(polynorbornene-g-polyethylene oxide)-b-(polynorbornene-g-bromoethane) (PNPS-b-PNPEO-b-PNBr), are designed and synthesized for fabrication of the positively charged porous spheres through self-assembly and in situ quaternization during an organized spontaneous emulsification (OSE) process. Pore diameter as well as charge density increase with the increase of PNBr content, resulting in a significant increase of loading density from 4.79 to 22.5 ng µg-1 within the spheres. This work provides a general strategy for efficient loading and encapsulation of DNA, which may be extended to a variety of different areas for different real applications.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Polietilenoglicóis / Polímeros Idioma: En Revista: Macromol Rapid Commun Ano de publicação: 2023 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Polietilenoglicóis / Polímeros Idioma: En Revista: Macromol Rapid Commun Ano de publicação: 2023 Tipo de documento: Article