Your browser doesn't support javascript.
loading
The aging behavior of degradable plastic polylactic acid under the interaction of environmental factors.
Jiang, Hui; Wang, Yiqun; Sun, Jiaoxia; Mao, Yufeng; Que, Sisi; Lin, Yulian; Huang, Yuanyuan; Lei, Xiaoling.
Afiliação
  • Jiang H; Key Laboratory of Hydraulic and Waterway Engineering of the Ministry of Education, School of River and Ocean Engineering, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Wang Y; Chongqing Engineering Laboratory of Environmental Hydraulic Engineering, Chongqing Municipal Development and Reform Commission, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Sun J; Key Laboratory of Hydraulic and Waterway Engineering of the Ministry of Education, School of River and Ocean Engineering, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Mao Y; Chongqing Engineering Laboratory of Environmental Hydraulic Engineering, Chongqing Municipal Development and Reform Commission, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Que S; Key Laboratory of Hydraulic and Waterway Engineering of the Ministry of Education, School of River and Ocean Engineering, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Lin Y; Chongqing Engineering Laboratory of Environmental Hydraulic Engineering, Chongqing Municipal Development and Reform Commission, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Huang Y; Key Laboratory of Hydraulic and Waterway Engineering of the Ministry of Education, School of River and Ocean Engineering, Chongqing Jiaotong University, Chongqing, 400074, China.
  • Lei X; Chongqing Engineering Laboratory of Environmental Hydraulic Engineering, Chongqing Municipal Development and Reform Commission, Chongqing Jiaotong University, Chongqing, 400074, China.
Environ Geochem Health ; 46(5): 163, 2024 Apr 09.
Article em En | MEDLINE | ID: mdl-38592574
ABSTRACT
Microplastics leaching from aging biodegradable plastics pose potential environmental threats. This study used response surface methodology (RSM) to investigate the impact of temperature, light, and humidity on the aging characteristics of polylactic acid (PLA). Key evaluation metrics included the C/O ratio, functional groups, crystallinity, surface topography, and mechanical properties. Humidity was discovered to have the greatest effect on the ageing of PLA, followed by light and temperature. The interactions between temperature and light, as well as humidity and sunlight, significantly impact the aging of PLA. XPS analysis revealed PLA underwent aging due to the cleavage of the ester bond (O-C=O), resulting in the addition of C=O and C-O. The aging process of PLA was characterized by alterations in surface morphology and augmentation in crystallinity, resulting in a decline in both tensile strength and elongation. These findings might offer insights into the aging behavior of degradable plastics under diverse environmental conditions.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Plásticos / Ésteres Idioma: En Revista: Environ Geochem Health Assunto da revista: QUIMICA / SAUDE AMBIENTAL Ano de publicação: 2024 Tipo de documento: Article País de afiliação: China

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Plásticos / Ésteres Idioma: En Revista: Environ Geochem Health Assunto da revista: QUIMICA / SAUDE AMBIENTAL Ano de publicação: 2024 Tipo de documento: Article País de afiliação: China