Oxygen Substitution to Enhance Chemo-Mechanical Stability at the Cathode-Sulfide Electrolyte Interface in All-Solid-State Batteries.
Hwang, Taesoon; Bae, Jong-Hyuk; Lee, So-Ri; Park, Heetaek; Park, Jun-Woo; Ha, Yoon-Cheol; Lee, You-Jin; Cho, Kyeongjae.
Afiliação
  • Hwang T; Department of Materials Science and Engineering, University of Texas at Dallas, Richardson, Texas 75080-3021, United States.
  • Bae JH; Next Generation Battery Research Center, Korea Electrotechnology Research Institute (KERI) 12, Jeongiui-gil, Seongsan-gu, Changwon-si 51543, Republic of Korea.
  • Lee SR; Next Generation Battery Research Center, Korea Electrotechnology Research Institute (KERI) 12, Jeongiui-gil, Seongsan-gu, Changwon-si 51543, Republic of Korea.
  • Park H; Next Generation Battery Research Center, Korea Electrotechnology Research Institute (KERI) 12, Jeongiui-gil, Seongsan-gu, Changwon-si 51543, Republic of Korea.
  • Park JW; Next Generation Battery Research Center, Korea Electrotechnology Research Institute (KERI) 12, Jeongiui-gil, Seongsan-gu, Changwon-si 51543, Republic of Korea.
  • Ha YC; Next Generation Battery Research Center, Korea Electrotechnology Research Institute (KERI) 12, Jeongiui-gil, Seongsan-gu, Changwon-si 51543, Republic of Korea.
  • Lee YJ; Next Generation Battery Research Center, Korea Electrotechnology Research Institute (KERI) 12, Jeongiui-gil, Seongsan-gu, Changwon-si 51543, Republic of Korea.
  • Cho K; Department of Materials Science and Engineering, University of Texas at Dallas, Richardson, Texas 75080-3021, United States.
ACS Nano ; 18(34): 23320-23330, 2024 Aug 27.
Article em En | MEDLINE | ID: mdl-39151093
ABSTRACT
The high interface resistance at the cathode-sulfide electrolyte interface is still a crucial drawback in an all-solid-state battery, unlike the initial expectation that the all-solid-state interface would enhance electrochemical stability by reducing side reactions at the interface. In this study, we examined the fundamental mechanism of unexpected reactions at the interface of LiNi0.8Co0.1Mn0.1O2 (NCM811) and argyrodite (Li6PS5Br0.5Cl0.5, LPSBC) sulfide solid electrolytes based on the combined method of multiscale simulations and electrochemical experiments. The high interface resistance originates from the formation of a passivating layer at the interface combined with irregular atomic and electronic structures, Li depletion, mutual element exchange, and mechanical contact loss between the oxide cathode and sulfide solid electrolyte. We also confirmed that these side reactions were suppressed by O substitutions to sulfide solid electrolyte (LPSOBC), and then the chemo-mechanical stability of the all-solid battery was enhanced by alleviating the side reactions at the interface. This study provides rational insights into the design of an interface for all-solid-state batteries.