High-voltage LiNi0.5Mn1.5O4 (LNMO) spinel oxides are highly promising cobalt-free cathode materials to cater to the surging demand for lithium-ion batteries (LIBs). However, commercial application of LNMOs is still challenging despite decades of research. To address the challenge, the understanding of their crystallography and structural evolutions during synthesis and electrochemical operation is critical. This review aims to illustrate and to update the fundamentals of crystallography, phase transition mechanisms, and electrochemical behaviors of LNMOs. First, the research history of LNMO and its development into a LIB cathode material is outlined. Then the structural basics of LNMOs including the classic and updated views of the crystal polymorphism, interconversion between the polymorphs, and structure-composition relationship is reviewed. Afterward, the phase transition mechanisms of LNMOs that connect structural and electrochemical properties are comprehensively discussed from fundamental thermodynamics to operando dynamics at intra- and inter-particle levels. In addition, phase evolutions during overlithiation as well as thermal-/electrochemical-driven phase transformations of LNMOs are also discussed. Finally, recommendations are offered for the further development of LNMOs as well as other complex materials to unlock their full potential for future sustainable and powerful batteries.

2.
ACS Appl Mater Interfaces ; 15(51): 59319-59328, 2023 Dec 27.
Artigo em Inglês | MEDLINE | ID: mdl-38085792

RESUMO

Li-ion battery cathode active materials obtained from different sources or preparation methods often exhibit broadly divergent performance and stability despite no obvious differences in morphology, purity, and crystallinity. We show how state-of-the-art, commercial, nominally single crystalline LiNi0.6Mn0.2Co0.2O2 (NMC-622) particles possess extensive internal nanostructure even in the pristine state. Scanning X-ray diffraction microscopy reveals the presence of interlayer strain gradients, and crystal bending is attributed to oxygen vacancies. Phase contrast X-ray nano-tomography reveals two different kinds of particles, welded/aggregated, and single crystal like, and emphasizes the intra- and interparticle heterogeneities from the nano- to the microscale. It also detects within the imaging resolution (100 nm) substantial quantities of nanovoids hidden inside the bulk of two-thirds of the overall studied particles (around 3000), with an average value of 12.5%v per particle and a mean size of 148 nm. The powerful combination of both techniques helps prescreening and quantifying the defective nature of cathode material and thus anticipating their performance in electrode assembly/battery testing.

3.
Nat Commun ; 14(1): 6975, 2023 Nov 01.
Artigo em Inglês | MEDLINE | ID: mdl-37914690

RESUMO

Lithiation dynamics and phase transition mechanisms in most battery cathode materials remain poorly understood, because of the challenge in differentiating inter- and intra-particle heterogeneity. In this work, the structural evolution inside Li1-xMn1.5Ni0.5O4 single crystals during electrochemical delithiation is directly resolved with operando X-ray nanodiffraction microscopy. Metastable domains of solid-solution intermediates do not appear associated with the reaction front between the lithiated and delithiated phases, as predicted by current phase transition theory. Instead, unusually persistent strain gradients inside the single crystals suggest that the shape and size of solid solution domains are instead templated by lattice defects, which guide the entire delithiation process. Morphology, strain distributions, and tilt boundaries reveal that the (Ni2+/Ni3+) and (Ni3+/Ni4+) phase transitions proceed through different mechanisms, offering solutions for reducing structural degradation in high voltage spinel active materials towards commercially useful durability. Dynamic lattice domain reorientation during cycling are found to be the cause for formation of permanent tilt boundaries with their angular deviation increasing during continuous cycling.