Your browser doesn't support javascript.
loading
Comparison of the Effects of Various Methods Used to Remove Adhesive from Tooth Surfaces on Surface Roughness and Temperature Changes in the Pulp Chamber.
Amasyali, Mihri; Sabuncuoglu, Fidan Alakus; Ersahan, Seyda; Oktay, Elif Aybala.
Afiliação
  • Amasyali M; University of Health Sciences Gülhane Training and Research Hospital, Istanbul, Turkey.
  • Sabuncuoglu FA; Department of Orthodontics, University of Health Sciences School of Dentistry, Ankara, Turkey.
  • Ersahan S; Department of Orthodontics, University of Health Sciences School of Dentistry, Ankara, Turkey.
  • Oktay EA; Department of Endodontics, Istanbul Medipol University School of Dentistry, Istanbul, Turkey.
Turk J Orthod ; 32(3): 132-138, 2019 Sep.
Article em En | MEDLINE | ID: mdl-31565687
ABSTRACT

OBJECTIVE:

The purpose of the present study was to compare the effects of three methods of removing adhesive on enamel surface roughness and dental pulp temperature.

METHODS:

Ninety human maxillary premolars were randomly divided into three groups (n=30) according to the type of adhesive clean-up procedure aluminum oxide-based burs, erbium-doped yttrium aluminum garnet (ErYAG) laser, and tungsten carbide bur. The surface roughness of enamel was measured using a non-contact optical profilometer. After the first readings of surface roughness were measured (T1), orthodontic brackets were attached to the enamel surface with composite. The brackets on the teeth were debonded using bracket removal pliers. The residue of adhesive was eliminated from the enamel surface of the teeth by different procedures in each group. While removing adhesive from the tooth surface, the intrapulpal temperature rise was simultaneously measured using a thermocouple. One-way ANOVA and post-hoc Tukey HSD tests were used to analyze data with a significance level set at 0.05.

RESULTS:

The highest roughness average (Ra) values were observed for the ErYAG laser group, with a significant difference with the aluminum oxide bur group and tungsten carbide bur group (p<0.001). Ra values for the aluminum oxide bur group were significantly lower than those for the other groups (p<0.001). Comparing the thermal changes in each group showed a significant decrease in the ErYAG laser group, but a significant increase in two other groups.

CONCLUSION:

Within the limitations of the present study, one-step finisher and polisher bur created the smoothest enamel surface, whereas ErYAG laser the roughest. Tungsten carbide and aluminum oxide-based burs generated more heat than ErYAG laser.