Your browser doesn't support javascript.
loading
Stability under humidity, UV-light and bending of AZO films deposited by ALD on Kapton.
Marques, A C; Faria, J; Perdigão, P; Faustino, B M M; Ritasalo, Riina; Costabello, Katiuscia; da Silva, R C; Ferreira, I.
Afiliação
  • Marques AC; CENIMAT/I3N, Departamento de Ciência dos Materiais, Faculdade de Ciências e Tecnologia, Universidade Nova de Lisboa, Caparica, 2829-516, Portugal. acl.marques@fct.unl.pt.
  • Faria J; CENIMAT/I3N, Departamento de Ciência dos Materiais, Faculdade de Ciências e Tecnologia, Universidade Nova de Lisboa, Caparica, 2829-516, Portugal.
  • Perdigão P; CENIMAT/I3N, Departamento de Ciência dos Materiais, Faculdade de Ciências e Tecnologia, Universidade Nova de Lisboa, Caparica, 2829-516, Portugal.
  • Faustino BMM; CENIMAT/I3N, Departamento de Ciência dos Materiais, Faculdade de Ciências e Tecnologia, Universidade Nova de Lisboa, Caparica, 2829-516, Portugal.
  • Ritasalo R; Picosun Oy Masalantie 365, FI-02430, Masala, Finland.
  • Costabello K; GRINP Srl, via De Francisco 123, 10036, Settimo T.se, TO, Italy.
  • da Silva RC; IPFN-IST/UL, Instituto de Plasmas e Fusão Nuclear, Instituto Superior Técnico, Universidade de Lisboa, Estrada Nacional 10, 2695-066, Bobadela, Portugal.
  • Ferreira I; CENIMAT/I3N, Departamento de Ciência dos Materiais, Faculdade de Ciências e Tecnologia, Universidade Nova de Lisboa, Caparica, 2829-516, Portugal.
Sci Rep ; 9(1): 17919, 2019 Nov 29.
Article em En | MEDLINE | ID: mdl-31784687
ABSTRACT
Aluminium doped zinc oxide (AZO) films were grown by Atomic Layer Deposition (ALD) on yellow Kapton and transparent Kapton (type CS) substrates for large area flexible transparent thermoelectric applications, which performance relies on the thermoelectric properties of the transparent AZO films. Therefore, their adhesion to Kapton, environmental and bending stability were accessed. Plasma treatment on Kapton substrates improved films adhesion, reduced cracks formation, and enhanced electrical resistance stability over time, of importance for long term thermoelectric applications in external environment. While exposure to UV light intensity caused the films electrical resistance to vary, and therefore their maximum power density outputs (0.3-0.4 mW/cm3) for a constant temperature difference (∼10 °C), humidity exposure and consecutive bending up to a curvature radius above the critical one (∼18 mm) not. Testing whether the films can benefit from encapsulation revealed that this can provide extra bending stability and prevent contacts deterioration in the long term.