Bond strengths of three-step etch-and-rinse adhesives to silane contaminated dentin.
Soontornvatin, Vasavat; Prasansuttiporn, Taweesak; Thanatvarakorn, Ornnicha; Jittidecharaks, Sumana; Hosaka, Keiichi; Foxton, Richard M; Nakajima, Masatoshi.
Afiliação
  • Soontornvatin V; Dentist, Dental Section, Nongsung Hospital.
  • Prasansuttiporn T; Master of Science Program in Dentistry, Faculty of Dentistry, Chiang Mai University.
  • Thanatvarakorn O; Department of Restorative Dentistry and Periodontology, Faculty of Dentistry, Chiang Mai University.
  • Jittidecharaks S; Center of Excellence in Materials Science and Technology, Chiang Mai University.
  • Hosaka K; Faculty of Dentistry, Bangkokthonburi University.
  • Foxton RM; Department of Restorative Dentistry and Periodontology, Faculty of Dentistry, Chiang Mai University.
  • Nakajima M; Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University.
Dent Mater J ; 40(2): 385-392, 2021 Mar 31.
Article em En | MEDLINE | ID: mdl-33208575
ABSTRACT
This study aimed to evaluate the effect of silane coupling agent contamination on the microtensile bond strength (µTBS) of 3-step etch-and-rinse adhesives on dentin. Flat occlusal dentin surfaces were prepared and randomly divided into 8 groups (n=20) based on the tested adhesives; Scotchbond Multi-purpose or Optibond FL, with contamination of an experimental silane (2 vol% of 3-m ethacryloxypropyltrimethoxysilane at pH 4.5) before acid-etching, after-etching or after-priming; while the groups without silane contamination served as controls. µTBS data were analyzed by two-way ANOVA and Tukey's HSD tests at a significance level of 0.05. Additional specimens of contaminated dentin were used to analyze changes in the organic molecules by Fourier transform infrared spectroscopy (FTIR). Silane contamination before acid-etching did not significantly change µTBS (p>0.05), but contamination after-etching and after-priming significantly decreased µTBS of both adhesives (p<0.05). Silane contamination had an adverse effect on the dentin bond strength of 3-step etch-and-rinse adhesives especially after-priming.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Colagem Dentária / Adesivos Dentinários Idioma: En Ano de publicação: 2021 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Colagem Dentária / Adesivos Dentinários Idioma: En Ano de publicação: 2021 Tipo de documento: Article