Your browser doesn't support javascript.
loading
Influence of ER-CR-YSGG Laser and Photodynamic Therapy on the Dentin Bond Integrity of Nano-Hydroxyapatite Containing Resin Dentin Adhesive: SEM-EDX, Micro-Raman, Micro-Tensile, and FTIR Evaluation.
Aljamhan, Abdullah S; Alrefeai, Mohammad H; Alhabdan, Alhanouf; Alhusseini, Sarah A; Farooq, Imran; Vohra, Fahim; Naseem, Mustafa; Alkhudhairy, Fahad.
Afiliação
  • Aljamhan AS; Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
  • Alrefeai MH; Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
  • Alhabdan A; Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
  • Alhusseini SA; Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
  • Farooq I; Faculty of Dentistry, University of Toronto, Toronto, ON M5G 1G6, Canada.
  • Vohra F; Prosthetic Dental Science, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
  • Naseem M; Department of Community and Preventive Dental Sciences, Dow International Dental College, Karachi 74200, Pakistan.
  • Alkhudhairy F; Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.
Polymers (Basel) ; 13(12)2021 Jun 08.
Article em En | MEDLINE | ID: mdl-34201060
ABSTRACT
The study aimed to analyze the effect of the addition of nano-hydroxyapatite (nano-HA) particles on the mechanical properties of experimental adhesive (EA). Furthermore, dentin interaction of EA (without nano-HA) and EA with nano-HA (hereon referred to as HA-10%) were also investigated and equated. Methods consisting of scanning electron microscopy (SEM)-energy-dispersive X-ray spectroscopy (EDX), micro-Raman spectroscopy, micro-tensile bond strength (µTBS) test, and Fourier transform infrared (FTIR) spectroscopy were employed to study nano-HA particles shape, dentin bond strength, degree of conversion (DC), and adhesive-dentin interaction. Ninety teeth (N = 90) were collected, and pre-bonding, conditioning of dentin was performed utilizing phosphoric acid (H3PO4) etching, photodynamic therapy (PDT), and ER-CR-YSGG (ECY) laser. The teeth were set to form bonded specimens using two adhesives. Nano-HA particles were spherical-shaped, and EDX confirmed the presence of oxygen, calcium, and phosphorus. Micro-Raman spectroscopy revealed distinct phosphate and carbonate peaks for nano-HA. The µTBS test demonstrated highest values for HA-10% group on the H3PO4 conditioned dentin. The greatest DC was observed for the EA group. The addition of nano-HA-10 wt.% particles in dentin adhesive resulted in improved bond strength. The incorporation also demonstrated acceptable DC (although lower than EA group), suitable dentin interaction, and resin tag formation.