Your browser doesn't support javascript.
loading
Photocatalytic solid-phase degradation of polyethylene with fluoride-doped titania under low consumption ultraviolet radiation.
Díez, Aida M; Pazos, Marta; Sanromán, M Ángeles; Naranjo, Helen Valencia; Mayer, Joachim; Kolen'ko, Yury V.
Afiliação
  • Díez AM; Nanochemistry Research Group, International Iberian Nanotechnology Laboratory (INL), Braga, Portugal; CINTECX, Universidade de Vigo, Grupo de Bioingeniería y Procesos Sostenibles, Departamento de Ingeniería Química, Campus Lagoas-Marcosende, 36310 Vigo, Spain. Electronic address: adiez@uvigo.gal.
  • Pazos M; CINTECX, Universidade de Vigo, Grupo de Bioingeniería y Procesos Sostenibles, Departamento de Ingeniería Química, Campus Lagoas-Marcosende, 36310 Vigo, Spain.
  • Sanromán MÁ; CINTECX, Universidade de Vigo, Grupo de Bioingeniería y Procesos Sostenibles, Departamento de Ingeniería Química, Campus Lagoas-Marcosende, 36310 Vigo, Spain.
  • Naranjo HV; Central Facility for Electron Microscopy (GFE), RWTH Aachen University, D-52074 Aachen, Germany.
  • Mayer J; Central Facility for Electron Microscopy (GFE), RWTH Aachen University, D-52074 Aachen, Germany.
  • Kolen'ko YV; Nanochemistry Research Group, International Iberian Nanotechnology Laboratory (INL), Braga, Portugal.
J Environ Manage ; 329: 117044, 2023 Mar 01.
Article em En | MEDLINE | ID: mdl-36584507
ABSTRACT
Photodegradation of plastic in solid-phase requires the polymer to be composited with an efficient photocatalyst. We report herein the successful synthesis and characterization of fluoride-doped-TiO2 and its applicability, for the first time, on solid-phase photodegradation of polyethylene films. Nearly half weight loss of polyethylene, containing only 2% of the photocatalyst, is eliminated after three weeks of ultraviolet A radiation using a low consumption light emitting diode lamp, defeating previously reported data. The half-life time of the plastic was around 3 weeks, highlighting the viability of this process for real applications. Results were compared to raw PE and PE composite with well-known TiO2, resulting in, respectively, 0 and 26% of weight loss. The degradation process was monitored by optical microscopy, scanning electron microscopy, X-ray diffraction, thermogravimetric analysis, Fourier transform infrared and X-ray photoelectron spectroscopy, which revealed the formation of plastic cracks, loss of polyethylene crystallinity and thus stability, the oxidation of C-H bonds and the oxidized state of the surface compounds during photodegradation. The obtained results open a path for the future production of cleaner and self-photodegradable plastics, where the photocatalyst would be introduced in all the manufactured plastics, making possible the quicker photodegradation of the plastics that end up on the environment and the plastics reaching wastewater treatment plants.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Raios Ultravioleta / Polietileno Idioma: En Ano de publicação: 2023 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Raios Ultravioleta / Polietileno Idioma: En Ano de publicação: 2023 Tipo de documento: Article