Your browser doesn't support javascript.
loading
Study of the Durability of Membrane Electrode Assemblies in Various Accelerated Stress Tests for Proton-Exchange Membrane Water Electrolysis.
Su, Zhengquan; Liu, Jun; Li, Pengfei; Liang, Changhao.
Afiliação
  • Su Z; Institute of Physical Science and Information Technology, Anhui University, Hefei 230601, China.
  • Liu J; Key Laboratory of Materials Physics, Anhui Key Laboratory of Nanomaterials and Nanotechnology, Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031, China.
  • Li P; Key Laboratory of Materials Physics, Anhui Key Laboratory of Nanomaterials and Nanotechnology, Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031, China.
  • Liang C; Key Laboratory of Materials Physics, Anhui Key Laboratory of Nanomaterials and Nanotechnology, Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031, China.
Materials (Basel) ; 17(6)2024 Mar 14.
Article em En | MEDLINE | ID: mdl-38541484
ABSTRACT
In this work, we focus on the degradation of membrane electrode assemblies (MEAs) in proton-exchange membrane water electrolysis (PEMWE) induced by different accelerated stress tests (ASTs), including constant-current mode, square-wave mode, and solar photovoltaic mode. In constant-current mode, at continuous testing for 600 h at 80 °C, a degradation of operating voltage increased by the enhanced current density from 22 µV/h (1 A/cm2) to 50 µV/h (3 A/cm2). In square-wave mode, we found that in the narrow fluctuation range (1-2 A/cm2), the shorter step time (2 s) generates a higher degradation rate of operating voltage, but in the wide fluctuation range (1-3 A/cm2), the longer step time (22 s) induces a faster operating voltage rise. In the solar photovoltaic mode, we used a simulation of 11 h sunshine duration containing multiple constant-current and square-wave modes, which is closest to the actual application environment. Over 1400 h ASTs, the solar photovoltaic mode lead to the most serious voltage rise of 87.7 µV/h. These results are beneficial to understanding the durability of the PEM electrolyzer and optimizing the components of MEAs, such as catalysts, membranes, and gas diffusion layers.