Effect of hydrofluoric acid and self-etch ceramic primers on the flexural strength and fatigue resistance of glass ceramics: A systematic review and meta-analysis of in vitro studies.
Moreira, Paulo Matias; Carvalho, Gabriela Luiza Moreira; de Castro Albuquerque, Rodrigo; André, Carolina Bosso.
Afiliação
  • Moreira PM; Department of Restorative Dentistry, School of Dentistry, Federal University of Minas Gerais, Belo Horizonte, MG, Brazil.
  • Carvalho GLM; Department of Restorative Dentistry, School of Dentistry, Federal University of Minas Gerais, Belo Horizonte, MG, Brazil.
  • de Castro Albuquerque R; Department of Restorative Dentistry, School of Dentistry, Federal University of Minas Gerais, Belo Horizonte, MG, Brazil.
  • André CB; Department of Restorative Dentistry, School of Dentistry, Federal University of Minas Gerais, Belo Horizonte, MG, Brazil.
Jpn Dent Sci Rev ; 60: 198-210, 2024 Dec.
Article em En | MEDLINE | ID: mdl-39027733
ABSTRACT
This systematic review evaluated the effect of different hydrofluoric acid (HF) etching regimens and a self-etch ceramic primer (SECP) on the flexural strength (FS) and fatigue failure load (FFL) of glass-ceramic materials.The identification of relevant studies was conducted by two authors in five databases PubMED, Scopus, Web Of Science, LILACS and Virtual Health Library (BVS) until July 2022 with no year limit. The analysis was conducted in RevMan 5.4.1 Software (Cochrane Collaboration) using Random effect model at 5 %. The risk of bias of the included studies were assessed. From the 5349 articles identified, 34 were included for quantitative analysis. Meta-analysis showed that for predominantly glassy ceramics, etching with HF 5 % had no significant impact on FS, however, HF acid etching with concentrations greater than 5 % negatively impacted FS. For lithium disilicate glass-ceramics (LDGC) HF acid etching, negatively influenced FS, while increasing the FFL. HF etching negatively affected FS of hybrid ceramics. The self-etch ceramic primer and HF acid etching showed a similar impact on FFL and FS. This meta-analysis indicates that the impact of SECP and HF acid etching on the mechanical behavior of glass ceramics is material-dependent.