This study investigates the possibility of recovering nickel from the spent catalyst (NiO/Al2O3) resulting from the steam reforming process to produce water gas (H2/H2O) in many industries. In the extraction process, nickel is recovered as sulfate using sulfuric acid as a solvent. The considered parameters affecting nickel recovery were acid concentration, temperature and time of digestion solid:liquid ratio, particle size and stirring rate. Nickel was to be directly recovered as a sulfate salt by direct crystallization method. The conversion was 99% at 50% sulfuric acid concentration, solid: liquid ratio (1:12) by weight, particle size less than 500 micron for more than 5 h and 800 rpm at 100 degrees C.


Assuntos
Conservação dos Recursos Naturais , Níquel/química , Catálise , Gases , Resíduos Industriais , Solventes , Temperatura , Água
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA