1.
Materials (Basel) ; 16(3)2023 Jan 30.
Artigo em Inglês | MEDLINE | ID: mdl-36770186

RESUMO

In this paper, we discuss the preparation of Li-doped ZnO nanostructures through combustion and report on their structural, morphological, optical, and electrocatalysis properties. X-ray diffraction analyses show that the samples have a structure crystallized into the usual hexagonal wurtzite ZnO structure according to the P63mc space group. The scanning electron microscope images conceal all samples' nanosphere bundles and aggregates. The reflectance spectra analysis showed that the direct bandgap values varied from 3.273 eV (for pure ZnO, i.e., ZnL1) to 3.256 eV (for high Li-doped ZnO). The measured capacitance concerning frequency has estimated the variation of dielectric constant, dielectric loss, and AC conductivity against AC electric field frequency. The dielectric constant variations and AC conductivity are analyzed and discussed by well-known models such as Koop's phenomenological theory and Jonscher's law. The Raman spectra have been recorded and examined for the prepared samples. Rhodamine B was electro-catalytically degraded in all prepared samples, with the fastest time for ZnL5 being 3 min.

2.
Environ Sci Pollut Res Int ; 29(13): 19109-19131, 2022 Mar.
Artigo em Inglês | MEDLINE | ID: mdl-34713401

RESUMO

In this proposed study, erbium (Er3+)-doped ZnO nanocomposites were prepared through the effective, basic, and green combustion method. The significant effects of Er dopants on the structural, morphological features, dielectric, and optical behaviors of the pure ZnO matrix as well as Er2O3-ZnO nanostructured materials were investigated applying X-ray diffraction (XRD), scanning electron microscopy (SEM), Fourier transformation infrared (FT-IR) spectroscopy, and UV-Vis spectrophotometer techniques. These results showed that the synthesized Er2O3-ZnO nanocomposites are well polycrystalline. The Er2O3-ZnO nanocomposites are almost uniformly distributed on the surface morphologies. Furthermore, UV-Vis diffuse reflectance spectroscopy, AC electrical conductivity, and dielectric properties' current-voltage characteristics were utilized to examine the influence of erbium doping on the optical properties, energy bandgaps of the proposed Er2O3-ZnO nanostructured powder. The tested nano-samples were applied for the visible light photodegradation of p-chlorophenol(4-CP) and p-nitrophenol (4-NP). The Er-doped ZnO ratio affects the photocatalytic activity of the ZnO matrix. This current research substantiated that more than 99.5% of 4-CP and 4-NP were photodegraded through 30 min of irradiation. Four times, the Er:ZnO nanocatalysts were used and still displayed an efficiency of more than 96.5% for 4-CP and 4-NP degradations in the specified period of 30 min. The as-prepared Er2O3-ZnO nanostructures are considered novel potential candidates in broad nano-applications from visible photocatalytic degradation of waste pollutants to the electronic varistor devices.


Assuntos
Purificação da Água , Óxido de Zinco , Catálise , Cerâmica , Eletrônica , Luz , Espectroscopia de Infravermelho com Transformada de Fourier , Óxido de Zinco/química
3.
Materials (Basel) ; 15(19)2022 Oct 02.
Artigo em Inglês | MEDLINE | ID: mdl-36234207

RESUMO

A lanthanum oxide (La2O3)-ZnO nanostructured material was synthesized in the proposed study with different La2O3 concentrations, 0.001 g to 5 g (named So to S7), using the combustion method. X-ray diffraction (XRD), scanning electron microscopy (SEM), and Fourier transformation infrared spectroscopy (FT-IR) were utilized for investigating the structure, morphology, and spectral studies of the La2O3- ZnO nanomaterials, respectively. The results obtained from previous techniques support ZnO's growth from crystalline to nanoparticles' fine structure by changing the concentrations of lanthanum oxide (La2O3) dopants in the host matrix. The percentage of ZnO doped with La- influences the ZnO photocatalytic activity. SEM analysis confirmed the grain size ranged between 81 and 138 nm. Furthermore, UV-Vis diffuse reflectance spectroscopy was performed to verify the effects of La2O3 dopants on the linear optical properties of the nano-composite oxides. There was a variation in the energy bandgaps of La2O3-ZnO nanocomposites, increasing the weight concentrations of lanthanum dopants. The AC electrical conductivity, dielectric properties, and current-voltage properties support the enactment of the electrical characteristics of the ZnO nanoparticles by adding La2O3. All the samples under investigation were used for photodegradation with Rhodamine B (RhB) and Methylene Blue (MB). In less than 30 min of visible light irradiation, S4 (0.5 g) La2O3-ZnO reached 99% of RhB and MB degradation activity. This study showed the best photocatalytic effect for RhB and MB degradation of 0.13 and 0.11 min-1 by 0.5 g La2O3-ZnO. Recycling was performed five times for the nanocatalysts that displayed up to 98 percent catalytic efficiency for RhB and MB degradation in 30 min. The prepared La2O3-ZnO nanostructured composites are considered novel candidates for various applications in biomedical and photocatalytic studies.

4.
Materials (Basel) ; 15(9)2022 May 01.
Artigo em Inglês | MEDLINE | ID: mdl-35591591

RESUMO

An efficient and environmentally friendly combustion technique was employed to produce ZnO nanopowders with different Eu concentrations (from 0.001 g to 5 g). The structural morphology of the Eu2O3-ZnO nanocomposites was examined using XRD, SEM, and infrared spectroscopy (FT-IR). In addition, UV-Vis diffuse reflectance spectroscopy was also used to investigate the effects of europium (Eu) dopant on the optical behaviors and energy bandgaps of nano-complex oxides. The photocatalytic degradation efficiency of phenol and methylene blue was investigated using all the prepared Eu2O3-ZnO nanostructured samples. Photocatalytic effectiveness increased when europium (Eu) doping ratios increased. After adding moderate Eu, more hydroxyl radicals were generated over ZnO. The best photocatalyst for phenol degradation was 1 percent Eu2O3-ZnO, while it was 0.5 percent Eu2O3-ZnO for methylene blue solutions. The obtained Eu2O3-doped ZnO nanostructured materials are considered innovative, promising candidates for a wide range of nano-applications, including biomedical and photocatalytic degradation of organic dyes and phenol.

5.
Nanomaterials (Basel) ; 12(7)2022 Mar 24.
Artigo em Inglês | MEDLINE | ID: mdl-35407178

RESUMO

The growth of the textile industry results in a massive accumulation of dyes on water. This enormous rise in pigments is the primary source of water pollution, affecting the aquatic lives and our ecosystem balance. This study aims to notify the fabrication of neodymium incorporated copper oxide (Nd2O3 doped CuO) nanoparticles by combustion method for effective degradation of dye, methylene blue (MB). X-ray diffraction (XRD), Field emission Scanning electron microscopy (FESEM), Zeta potential have been applied for characterization. Photocatalyst validity has been evaluated for methylene blue degradation (MB). Test conditions such as time of contact, H2O2, pH, and photo-Fenton have been modified to identify optimal degradation conditions. Noticeably, 7.5% Nd2O3 doped CuO nanoparticle demonstrated the highest photocatalytic efficiency, up to 90.8% in 80 min, with a 0.0227 min-1 degradation rate. However, the photocatalytic efficiency at pH 10 becomes 99% with a rate constant of 0.082 min-1. Cyclic experiments showed the Nd2O3 doped CuO nanoparticle's stability over repeated use. Scavenge hydroxyl radical species responsible for degradation using 7.5% Nd2O3 doped CuO nanoparticles have been investigated under visible irradiation.