RESUMO
Anion exchange membrane fuel cells (AEMFCs) and water electrolysis (AEMWE) show great application potential in the field of hydrogen energy conversion technology. However, scalable anion exchange membranes (AEMs) with desirable properties are still lacking, which greatly hampers the commercialization of this technology. Herein, we propose a series of novel multiblock AEMs based on ether-free poly(biphenyl ammonium-b-biphenyl phenyl)s (PBPA-b-BPPs) that are suitable for use in high performance AEMFC and AEMWE systems because of their well-formed microphase separation structures. The developed AEMs achieved outstanding OH- conductivity (162.2â mS cm-1 at 80 °C) with a low swelling ratio, good alkaline stability, and excellent mechanical durability (tensile strength >31â MPa and elongation at break >147 % after treatment in 2â M NaOH at 80 °C for 3750â h). A PBPA-b-BPP-based AEMFC demonstrated a remarkable peak power density of 2.41â W cm-2 and in situ durability for 330â h under 0.6â A cm-2 at 70 °C. An AEMWE device showed a promising performance (6.25â A cm-2 at 2â V, 80 °C) and outstanding in situ durability for 3250â h with a low voltage decay rate (<28â µV h-1 ). The newly developed PBPA-b-BPP AEMs thus show great application prospects for energy conversion devices.
RESUMO
Anion exchange membrane (AEM) fuel cells have gained significant interest in recent years due to their promising applications in cost-effective and environmentally friendly energy conversion. Among various factors that affect their performance, water content plays an important role in the conductivity and stability of AEMs. However, the effect of the hydration level on the microstructure of AEMs and the correlation between the microstructure and macroconductivity have not been systematically investigated. In this work, four AEMs, quaternary ammonia polysulfone, quaternary ammonia poly(N-methyl-piperidine-co-p-terphenyl) (QAPPT), and bromoalkyl-tethered poly(biphenyl alkylene)s PBPA and PBPA-co-BPP, have been studied by atomic force microscopy and electrochemical impedance spectroscopy to elucidate the correlation between the humidity-dependent surface microstructure and macroconductivity of the AEMs. We obtained phase images by atomic force microscopy and identified hydrophilic and hydrophobic domains by fitting the distribution curve of phase images, which reasonably distinguishes hydrophilic domains from hydrophobic domains of the membrane surface, and thus, the surface hydrophilic area ratio and average size could be quantitatively analyzed. The conductivities of the membranes were then measured by electrochemical impedance spectroscopy at various humidities. The joint results from atomic force microscopy and electrochemical measurements help clarify the effect of the hydration level on the microphase separation and ionic conduction of the membranes.
RESUMO
In order to separate palladium (II) from electroplating wastewaters, poly(4-vinylpyridine)-b-polysulfone-b-poly(4-vinylpyridine) (P4VP-PSF-P4VP) / polysulfone blend membranes were fabricated by combining non-solvent induced phase separation, surface segregation and self-assembly of block copolymer. Amphiphilic P4VP-PSF-P4VP was used as the membrane base material, which was synthesized by introducing the functional monomer of 4-vinylpyridine (4-VP), and polysulfone as the additive. Effects of blend ratio and 4-VP content on membrane performance, such as structure, hydrophilicity, pure water flux and adsorption capacity towards Pd (II), were investigated. The membranes exhibited dense surface structure and low roughness due to surface segregation and self-assembly of P4VP-PSF-P4VP. The presence of 4-VP increased hydrophilicity and water flux of membrane, and it also provided good adsorption capacity towards Pd (II) (up to 103.1⯱â¯5.15â¯mg/g). Further, the membrane was used to separate Pd (II) from simulated wastewaters during filtration. It showed good rejection ability and high selectivity towards Pd (II) in co-existence of Cu (II) and Ni (II), and selectivity coefficients of Pd/Cu and Pd/Ni are 41.9⯱â¯1.88 and 97.8⯱â¯4.32, respectively. In filtration process of actual electroplating wastewater, the membrane also exhibited excellent rejection performance (Pd (II) rejection reached up to 96.8⯱â¯2.71%). Perhaps it is suitable for future practice applications.