Measurement of shear bond strength to intact dentin.
Dent Mater J
; 29(2): 199-205, 2010 Mar.
Article
en En
| MEDLINE
| ID: mdl-20379031
Previously, we reported that the integrity of a resin composite restoration deteriorated when the dentin cavity wall was decalcified by conditioning. In this study, to evaluate the bonding between dentin adhesive and non-decalcified dentin surface, we experimented with a novel method of using a high-pressure water spray device to prepare smear layer-free dentin surfaces. When the smear layer was removed, shear bond strength significantly increased regardless of the removal method employed. Further, with glyceryl monomethacrylate (GM) priming, no significant differences in bond strength were observed among these smear layer removal methods: ethylenediamine tetraacetic acid (EDTA) conditioning, phosphoric acid conditioning, and removal by water spray. It was also found that GM priming was key to achieving marginal integrity, whereas contraction gap width increased with phosphoric acid conditioning. It was thus concluded that the efficacy of a dentin adhesive should be evaluated by consistently observing the contraction gap in three-dimensional cavities rather than by mere measurement of bond strength to a flat dentin surface.
Buscar en Google
Colección:
01-internacional
Banco de datos:
MEDLINE
Asunto principal:
Recubrimiento Dental Adhesivo
/
Recubrimientos Dentinarios
/
Dentina
Límite:
Humans
Idioma:
En
Revista:
Dent Mater J
Año:
2010
Tipo del documento:
Article
País de afiliación:
Japón