Your browser doesn't support javascript.
loading
A one-step process for multi-gradient wettability modification on a polymer surface.
Li, Xinxin; Mao, Xinyu; Li, Xudong; Liu, Chong; Li, Jingmin.
Afiliação
  • Li X; Department of Mechanical Engineering, Dalian University of Technology, Dalian, Liaoning, China. chongl@dlut.edu.cn.
  • Mao X; Department of Mechanical Engineering, Dalian University of Technology, Dalian, Liaoning, China. chongl@dlut.edu.cn.
  • Li X; Department of Mechanical Engineering, Dalian University of Technology, Dalian, Liaoning, China. chongl@dlut.edu.cn.
  • Liu C; Department of Mechanical Engineering, Dalian University of Technology, Dalian, Liaoning, China. chongl@dlut.edu.cn.
  • Li J; Department of Mechanical Engineering, Dalian University of Technology, Dalian, Liaoning, China. chongl@dlut.edu.cn.
Analyst ; 149(7): 2103-2113, 2024 Mar 25.
Article em En | MEDLINE | ID: mdl-38421308
ABSTRACT
The surface modification technique is applied in microfluidic devices to modify wettability and achieve different flow velocities. Currently available methods for poly(dimethylsiloxane) (PDMS) surfaces may reliably induce wettability changes, but only one area can be altered at a time. This work introduces the controlled gradient oxygen plasma modification (CGPM) technique, which layers several resin masks with varying porosities on top of the PDMS surface. Selective wettability of the PDMS surface can be achieved by varying the oxygen plasma density above the modified material's surface by manipulation of the porosity value. Through the implementation of the COMSOL plasma module, the impact of the mask's porosity, through-hole size, distribution, and distance from the PDMS surface on wettability was studied. The suggested CGPM approach was characterized by contact angle measurements. During the 25-second CGPM procedure, the PDMS surface's contact angle continually changed from 8.77° to 76.98°. An integrated microfluidic device was created and manufactured to identify D-dimers to illustrate this method. In comparison with standard oxygen plasma treatment, the D-dimer assay was finished in 10 minutes and had a dynamic range of 1-1000 ng mL-1, with a peak fluorescence signal augmentation of 78.3% and an average fluorescence intensity enhancement of 31.1%.