Your browser doesn't support javascript.
loading
Enhancing Zinc Electrode Stability Through Pre-Desolvation and Accelerated Charge Transfer via a Polyimide Interface for Zinc-Ion Batteries.
Lai, Chi-Yu; Liao, Yin-Song; Ku, Hao-Yu; Jao, Wen-Yang; Gull, Sanna; Chen, Han-Yi; Chou, Jyh-Pin; Hu, Chi-Chang.
Afiliação
  • Lai CY; Department of Chemical Engineering, National Tsing Hua University, Hsinchu, 300044, Taiwan.
  • Liao YS; Tsing Hua Interdisciplinary Program, National Tsing Hua University, Hsinchu, 300044, Taiwan.
  • Ku HY; Department of Chemical Engineering, National Tsing Hua University, Hsinchu, 300044, Taiwan.
  • Jao WY; Department of Chemical Engineering, National Tsing Hua University, Hsinchu, 300044, Taiwan.
  • Gull S; Department of Materials Science and Engineering, National Tsing Hua University, Hsinchu, 300044, Taiwan.
  • Chen HY; Department of Materials Science and Engineering, National Tsing Hua University, Hsinchu, 300044, Taiwan.
  • Chou JP; Department of Physics, National Changhua University of Education, Changhua, 50074, Taiwan.
  • Hu CC; Department of Chemical Engineering, National Tsing Hua University, Hsinchu, 300044, Taiwan.
Small ; : e2401713, 2024 May 01.
Article em En | MEDLINE | ID: mdl-38693076
ABSTRACT
Aqueous zinc-based energy storage devices possess superior safety, cost-effectiveness, and high energy density; however, dendritic growth and side reactions on the zinc electrode curtail their widespread applications. In this study, these issues are mitigated by introducing a polyimide (PI) nanofabric interfacial layer onto the zinc substrate. Simulations reveal that the PI nanofabric promotes a pre-desolvation process, effectively desolvating hydrated zinc ions from Zn(H2O)6 2+ to Zn(H2O)4 2+ before approaching the zinc surface. The exposed zinc ion in Zn(H2O)4 2+ provides an accelerated charge transfer process and reduces the activation energy for zinc deposition from 40 to 21 kJ mol-1. The PI nanofabric also acts as a protective barrier, reducing side reactions at the electrode. As a result, the PI-Zn symmetric cell exhibits remarkable cycling stability over 1200 h, maintaining a dendrite-free morphology and minimal byproduct formation. Moreover, the cell exhibits high stability and low voltage hysteresis even under high current densities (20 mA cm-2, 10 mAh cm-2) thanks to the 3D porous structure of PI nanofabric. When integrated into full cells, the PI-Zn||AC hybrid zinc-ion capacitor and PI-Zn||MnVOH@SWCNT zinc-ion battery achieve impressive lifespans of 15000 and 600 cycles with outstanding capacitance retention. This approach paves a novel avenue for high-performance zinc metal electrodes.