Response of human bone marrow-derived MSCs on triphasic Ca-P substrate with various HA/TCP ratio.
Bajpai, Indu; Kim, Duk Yeon; Kyong-Jin, Jung; Song, In-Hwan; Kim, Sukyoung.
Afiliación
  • Bajpai I; School of Materials Science and Engineering, Yeungnam University, 280 Daehak-Ro, Gyeongsan, Gyeoungbuk, 712-749, South Korea.
  • Kim DY; School of Materials Science and Engineering, Yeungnam University, 280 Daehak-Ro, Gyeongsan, Gyeoungbuk, 712-749, South Korea.
  • Kyong-Jin J; Department of Anatomy, College of Medicine, Yeungnam University, 317-1 Daemyung-Dong, 705-717, South Korea.
  • Song IH; Department of Anatomy, College of Medicine, Yeungnam University, 317-1 Daemyung-Dong, 705-717, South Korea.
  • Kim S; School of Materials Science and Engineering, Yeungnam University, 280 Daehak-Ro, Gyeongsan, Gyeoungbuk, 712-749, South Korea.
J Biomed Mater Res B Appl Biomater ; 105(1): 72-80, 2017 01.
Article en En | MEDLINE | ID: mdl-26415752
Calcium phosphates (Ca-P) are used commonly as artificial bone substitutes to control the biodegradation rate of an implant in the body fluid. This study examined the in vitro proliferation of human bone marrow-derived mesenchymal stem cells (hBMSCs) on triphasic Ca-P samples. For this aspect, hydroxyapatite (HA), dicalcium phosphate dehydrate (DCPD), and calcium hydroxide (Ca(OH)2 ) were mixed at various ratios, cold compacted, and sintered at 1250°C in air. X-ray diffraction showed that the ß-tricalcium phosphate (TCP) to α-TCP phase transformation increased with increasing DCPD/HA ratio. The micro-hardness deceased with increasing TCP content, whereas the mean grain size and porosity increased with increasing TCP concentration. To evaluate the in vitro degree of adhesion and proliferation on the HA/TCP samples, human BMSCs were incubated on the HA/TCP samples and analyzed by a cells proliferation assay, expression of the extracellular matrix (ECM) genes, such as α-smooth muscle actin (α-SMA) and fibronectin (FN), and FITC-phalloidin fluorescent staining. In terms of the interactions of human BMSCs with the triphasic Ca-P samples, H50T50 (Ca/P = 1.59) markedly enhanced cell spreading, proliferation, FN, and α-SMA compared with H100T0 (Ca/P = 1.67). Interestingly, these results show that among the five HA/TCP samples, H50T50 is the optimal Ca-P composition for in vitro cell proliferation. © 2015 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 72-80, 2017.
Asunto(s)
Palabras clave

Texto completo: 1 Colección: 01-internacional Asunto principal: Fosfatos de Calcio / Durapatita / Proliferación Celular / Células Madre Mesenquimatosas Límite: Humans Idioma: En Revista: J biomed mater res b appl biomater Asunto de la revista: ENGENHARIA BIOMEDICA Año: 2017 Tipo del documento: Article País de afiliación: Corea del Sur

Texto completo: 1 Colección: 01-internacional Asunto principal: Fosfatos de Calcio / Durapatita / Proliferación Celular / Células Madre Mesenquimatosas Límite: Humans Idioma: En Revista: J biomed mater res b appl biomater Asunto de la revista: ENGENHARIA BIOMEDICA Año: 2017 Tipo del documento: Article País de afiliación: Corea del Sur