Environ Technol ; 33(7-9): 995-1003, 2012.
Artigo em Inglês | MEDLINE | ID: mdl-22720426

RESUMO

Optimization of photocatalytic degradation of C.I. Reactive Green 19 (RG 19) under UV light irradiation using ceramic-coated TiO2 nanoparticles in a continuous circulation rectangular photoreactor was studied. The used catalyst was TiO2 Millennium PC-500 (crystallite mean size 8 nm) immobilized on ceramic plates. A central composite design was used for optimization of the UV/TiO2 process. Predicted values of decolorization efficiency were found to be in good agreement with experimental values (R2 = 0.97 and Adj-R2 = 0.91). Optimization results showed that maximum decolorization efficiency was achieved at the optimum conditions of: initial dye concentration 10 mg/L, UV light intensity 47.2 W/m2, flow rate 150 mL/min and reaction time 240 min. Photocatalytic mineralization of RG 19 was monitored by chemical oxygen demand (COD) decrease and changes in the UV-Vis spectrum.


Assuntos
Compostos de Diazônio/química , Fotólise , Titânio/química , Análise de Variância , Análise da Demanda Biológica de Oxigênio , Cerâmica , Corantes/química , Nanopartículas/química , Raios Ultravioleta
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA