Enhanced Photocatalytic Degradation by the Preparation of a Stable La-Doped FeTiO3 Photocatalyst: Experimental and DFT Study.
Luo, Xingrui; Zhu, Peng; Zeng, Jinming; Liang, Tongxiang; Qiu, Qingqing.
Affiliation
  • Luo X; Engineering Research Center for Hydrogen Energy Materials and Devices, College of Rare Earths, Jiangxi University of Science and Technology, 86 Hong Qi Road, Ganzhou 341000, People's Republic of China.
  • Zhu P; School of Chemistry and Chemical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, People's Republic of China.
  • Zeng J; Engineering Research Center for Hydrogen Energy Materials and Devices, College of Rare Earths, Jiangxi University of Science and Technology, 86 Hong Qi Road, Ganzhou 341000, People's Republic of China.
  • Liang T; Engineering Research Center for Hydrogen Energy Materials and Devices, College of Rare Earths, Jiangxi University of Science and Technology, 86 Hong Qi Road, Ganzhou 341000, People's Republic of China.
  • Qiu Q; Engineering Research Center for Hydrogen Energy Materials and Devices, College of Rare Earths, Jiangxi University of Science and Technology, 86 Hong Qi Road, Ganzhou 341000, People's Republic of China.
Inorg Chem ; 63(31): 14425-14437, 2024 Aug 05.
Article in En | MEDLINE | ID: mdl-39058345
ABSTRACT
The rapid photocarrier recombination limits the photocatalytic activity of iron titanate (FeTiO3) to be further improved. Developing novel approaches to inhibit the rapid recombination rate of the FeTiO3 photocatalysts is crucial for efficiently degrading pollutants in wastewater. Rare earth ions, with unique electron dispositions and large ion radii, could effectively inhibit photocarrier recombination. Herein, novel lanthanum (La)-doped FeTiO3 photocatalysts were designed and successfully synthesized. The photocatalytic performance of the 12 mol % La/FeTiO3 photocatalyst was superior in degrading tetracycline hydrochloride (TCH), methylene blue (MB), and brilliant blue (BB). These degradation rate constants (k) were 0.12358, 0.01357, and 0.03064 L mg-1 min-1, respectively, which were 12.83, 1.61, and 7.78 times that of pure FeTiO3. The photoelectronic tests and density functional theory (DFT) calculations revealed that the La 4f orbital forms an impurity energy level in the conduction band of FeTiO3. This level narrows the bandgap and acts as an electron acceptor, capturing photoexcited electrons and inhibiting the rapid recombination of photoexcited electron-hole pairs in FeTiO3. This work enhances the potential of FeTiO3 in the photocatalysis field and provides important insights into the efficient degradation of organic pollutants in wastewater.