Your browser doesn't support javascript.
loading
Adsorption and photocatalytic degradation of 2,4-dicholrophenol using surgical mask derived SMAC-Fe2O3 composite; adsorption isotherms, kinetics, thermodynamics.
Manojkumar, Utaiyachandran; Kaliannan, Durairaj; Balasubramanian, Balamuralikrishnan; Senthilkumar, Palaninaicker; Kamyab, Hesam; Chelliapan, Shreeshivadasan.
Afiliación
  • Manojkumar U; Department of Environmental Science, School of Energy and Environmental Sciences, Periyar University, Salem, Tamil Nadu, 636011, India.
  • Kaliannan D; Department of Environmental Science, School of Energy and Environmental Sciences, Periyar University, Salem, Tamil Nadu, 636011, India.
  • Balasubramanian B; Uniqdot Co., Ltd., 50 UNIST-Gil, Ulju-Gun, Ulsan, 44919, South Korea.
  • Senthilkumar P; Department of Food Science and Biotechnology, College of Life Science, Sejong University, Seoul, 05006, South Korea.
  • Kamyab H; Department of Environmental Science, School of Energy and Environmental Sciences, Periyar University, Salem, Tamil Nadu, 636011, India.
  • Chelliapan S; Department of Biomaterials, Saveetha Dental College and Hospital, Saveetha Institute of Medical and Technical Sciences, Chennai, 600 077, India. hesam_kamyab@yahoo.com.
Environ Sci Pollut Res Int ; 31(40): 52827-52840, 2024 Aug.
Article en En | MEDLINE | ID: mdl-39160408
ABSTRACT
Hybrid material of surgical mask activated carbon (SMAC) and Fe2O3 (SMAC-Fe2O3) composite was prepared by simple co-precipitation method and used as potential material for the remediation of 2,4-dicholrophenol (2,4-DCP). The XRD patterns exhibited the presence of SMAC and Fe2O3, FTIR spectrum showed the FeO-carbon stretching at the wavenumber from 400 to 550 cm-1. UV-Vis DRS results showed the band gap was 1.97 eV and 2.05 eV for SMAC-Fe2O3 and Fe2O3, respectively. The SEM images revealed that the Fe2O3 doped onto the fiber morphology of SMAC. The outcomes of the BET examination exhibited a surface area of 195 m2/g and a pore volume of 0.2062 cm3/g for the SMAC/Fe2O3 composite. The batch mode study shows the maximum adsorption and photocatalytic degradation efficacies which were 97% and 78%, respectively. The experimental data was studied with both linear and nonlinear adsorption isotherm and kinetics models. The nonlinear Langmuir isotherm and pseudo-second-order kinetics (PSOK) models have well fit compared with other models. The Langmuir maximum adsorption capacity (qmax) was found 161.60 mg/g. Thermodynamic analysis shows that the 2,4-DCP adsorption onto SMAC-Fe2O3 was a spontaneous and exothermic process. The PSOK assumes that the adsorption process was chemisorption. The photocatalytic degradation rate constant of 2,4-DCP was calculated using pseudo-first-order kinetics (PFOK) and the rate constant for SMAC-Fe2O3 and Fe2O3 were 0.859 × 10-2 min-1 and 0.616 × 10-2 min-1, correspondingly. In addition, the obtained composite exhibited good reusability after a few cycles. These results confirmed that SMAC-Fe2O3 composite is an effective adsorbent and photocatalyst for removing 2,4-DCP pollutants.
Asunto(s)
Palabras clave

Texto completo: 1 Bases de datos: MEDLINE Asunto principal: Termodinámica Idioma: En Revista: Environ Sci Pollut Res Int Asunto de la revista: SAUDE AMBIENTAL / TOXICOLOGIA Año: 2024 Tipo del documento: Article País de afiliación: India

Texto completo: 1 Bases de datos: MEDLINE Asunto principal: Termodinámica Idioma: En Revista: Environ Sci Pollut Res Int Asunto de la revista: SAUDE AMBIENTAL / TOXICOLOGIA Año: 2024 Tipo del documento: Article País de afiliación: India