1.
ACS Catal ; 14(13): 9850-9859, 2024 Jul 05.
Artigo em Inglês | MEDLINE | ID: mdl-38988652

RESUMO

We present here the synthesis and performance of dual-atom catalysts (DACs), analogous to well-known single-atom catalysts (SACs). DACs feature sites containing pairs of metal atoms and can outperform SACs due to their additional binding possibilities. Yet quantifying the improved catalytic activity in terms of proximity effects remains difficult, as it requires both high-resolution kinetic data and an understanding of the reaction pathways. Here, we use an automated bubble counter setup for comparing the catalytic performance of ceria-supported platinum SACs and DACs in ammonia borane hydrolysis. The catalysts were synthesized by wet impregnation and characterized using SEM, HAADF-STEM, XRD, XPS, and CO-DRIFTS. High-precision kinetic studies of ammonia borane hydrolysis in the presence of SACs show two temperature-dependent regions, with a transition point at 43 °C. Conversely, the DACs show only one regime. We show that this is because DACs preorganize both ammonia borane and water at the dual-atom active site. The additional proximal Pt atom improves the reaction rate 3-fold and enables faster reactions at lower temperatures. We suggest that the DACs enable the activation of the water-O-H bond as well as increase the hydrogen spillover effect due to the adjacent Pt site. Interestingly, using ammonia borane hydrolysis as a benchmark reaction gives further insight into hydrogen spillover mechanisms, above what is known from the CO oxidation studies.

2.
Catal Sci Technol ; 14(19): 5662-5670, 2024 Sep 30.
Artigo em Inglês | MEDLINE | ID: mdl-39156760

RESUMO

The local coordination environment of single atom catalysts (SACs) often determines their catalytic performance. To understand these metal-support interactions, we prepared Pt SACs on cerium dioxide (CeO2) cubes, octahedra and rods, with well-structured exposed crystal facets. The CeO2 crystals were characterized by SEM, TEM, pXRD, and N2 sorption, confirming the shape-selective synthesis, identical bulk structure, and variations in specific surface area, respectively. EPR, XPS, TEM and XANES measurements showed differences in the oxygen vacancy density following the trend rods > octahedra > cubes. AC-HAADF-STEM, XPS and CO-DRIFTS measurements confirmed the presence of only single Pt2+ sites, with different surface platinum surface concentrations. We then compared the performance of the three catalysts in ammonia borane hydrolysis. Precise monitoring of reaction kinetics between 30-80 °C gave Arrhenius plots with hundreds of data points. All plots showed a clear inflection point, the temperature of which (rods > octahedra > cubes) correlates to the energy barrier of ammonia borane diffusion to the Pt sites. These activity differences reflect variations in the - facet dependent - degree of stabilization of intermediates by surface oxygen lone pairs and surface-metal binding strength. Our results show how choosing the right macroscopic support shape can give control over single atom catalysed reactions on the microscopic scale.

3.
Adv Sci (Weinh) ; 10(4): e2206180, 2023 Feb.
Artigo em Inglês | MEDLINE | ID: mdl-36507566

RESUMO

Alkaline water electrolysis (AWE) is among the most developed technologies for green hydrogen generation. Despite the tremendous achievements in boosting the catalytic activity of the electrode, the operating current density of modern water electrolyzers is yet much lower than the emerging approaches such as the proton-exchange membrane water electrolysis (PEMWE). One of the dominant hindering factors is the high overpotentials induced by the gas bubbles. Herein, the bubble dynamics via creating the superaerophobic electrode assembly is optimized. The patterned Co-Ni phosphide/spinel oxide heterostructure shows complete wetting of water droplet with fast spreading time (≈300 ms) whereas complete underwater bubble repelling with 180° contact angle is achieved. Besides, the current collector/electrode interface is also modified by coating with aerophobic hydroxide on Ti current collector. Thus, in the zero-gap water electrolyzer test, a current density of 3.5 A cm-2 is obtained at 2.25 V and 85 °C in 6 m KOH, which is comparable with the state-of-the-art PEMWE using Pt-group metal catalyst. No major performance degradation or materials deterioration is observed after 330 h test. This approach reveals the importance of bubble management in modern AWE, offering a promising solution toward high-rate water electrolysis.

4.
Catal Sci Technol ; 13(7): 2255-2260, 2023 Apr 03.
Artigo em Inglês | MEDLINE | ID: mdl-37025647

RESUMO

Single-atom catalysts often show exceptionally high performance per metal loading. However, the isolated atom sites tend to agglomerate during preparation and/or high-temperature reaction. Here we show that in the case of Rh/Al2O3 this deactivation can be prevented by dissolution/exsolution of metal atoms into/from the support. We design and synthesise a series of single-atom catalysts, characterise them and study the impact of exsolution in the dry reforming of methane at 700-900 °C. The catalysts' performance increases with increasing reaction time, as the rhodium atoms migrate from the subsurface to the surface. Although the oxidation state of rhodium changes from Rh(iii) to Rh(ii) or Rh(0) during catalysis, atom migration is the main factor affecting catalyst performance. The implications of these results for preparing real-life catalysts are discussed.